Kodi Mungasankhe Bwanji Chipinda cha Electrode cha Stick?

Kuwotcherera ndi ntchito yofunika kwambiri popanga zinthu zambiri zopangidwa ndi chitsulo ndi aluminiyamu. Kulimba kwa kapangidwe kake konse komanso kupambana kwa polojekitiyi nthawi zambiri kumadalira mtundu wa chowotcherera. Chifukwa chake, kupatula zida zoyenera, muyeneranso kudziwa momwe zinthuzo ziyenera kulumikizidwa. Chimodzi mwa zinthu zomwe zimasinthasintha mu ndondomeko yonseyi ndi njira yowotcherera. Pachifukwa cha positi iyi, tingoyang'ana kwambiri pa kuwotcherera kwa arc ndi ma electrode ophimbidwa.

Kodi kuwotcherera kwa arc ndi manja n'chiyani?

Njira yonseyi ndi yosavuta. Ndi imodzi mwa njira zodziwika bwino zowotcherera. Imakhala kusungunula chivundikirocho pamodzi ndi electrode yogwiritsidwa ntchito ndi zinthu zowotcherera pogwiritsa ntchito arc yamagetsi. Ntchito zambiri zimachitika pamanja ndipo ubwino wa ntchitoyo umadalira luso la wowotcherera. Komabe, pali zinthu zofunika kuziganizira ngati mukufuna kugwira ntchito mwaukadaulo. Muyenera kuyang'ana, pakati pa zina:

gwero la mphamvu yolunjika komanso yosinthasintha, mwachitsanzo makina otchuka olumikizirana

chingwe chokhala ndi chogwirira cha elekitirodi

chingwe choponderezedwa pansi chokhala ndi chomangira cha electrode

mtundu wa chisoti ndi zinthu zina zowonjezera

Kupatula njira yowotcherera yokha, kusankha kwa dayamita ya electrode ya chinthu chowotcherera ndikofunikira kwambiri. Popanda iyo, kupanga weld yabwino sikungatheke. Kodi muyenera kulabadira chiyani kuti musangalale ndi zotsatira zake?

Kusankha m'mimba mwake wa electrode wa workpiece - muyenera kudziwa!

Kusankha kwa m'mimba mwake wa electrode pa chinthu cholumikizidwa mu njira ya MMA kumadalira makulidwe a weld kapena zinthu zomwe zikulumikizidwa. Malo omwe mukulumikiza nawonso ndi ofunikira. Kawirikawiri, zitha kuganiziridwa kuti m'mimba mwake muli pakati pa 1.6mm mpaka 6.0 mm. Ndikofunikira kuti m'mimba mwake wa electrode usapitirire makulidwe a zinthu zomwe mukufuna kulumikiza. Iyenera kukhala yaying'ono. M'mabuku okhudza kulumikiza mupeza zambiri zoti m'mimba mwake wa electrode iyenera kukhala yayikulu momwe mungathere. Kusunthaku ndikotsika mtengo kwambiri. Chifukwa chake, zinthu zokhala ndi makulidwe a 1.5 mm mpaka 2.5 mm zimalumikizidwa bwino ndi electrode yokhala ndi gawo la mtanda wa 1.6 mm. Nanga bwanji nthawi zina?

Zitsanzo za makulidwe a zinthu ndi kukula kwa ma electrode oyenera.

Kuti mudziwe bwino za kusankha kwa dayamita ya electrode pa ntchito, pansipa mupeza mndandanda waufupi wa makulidwe azinthu otchuka kwambiri komanso dayamita yabwino kwambiri ya electrode.

Kulemera kwa zinthu - M'mimba mwake wa electrode

1.5mm mpaka 2.5mm - 1.6mm

3.0mm mpaka 5.5mm - 2.5mm

4.0mm mpaka 6.5mm - 3.2mm

6.0mm mpaka 9.0mm - 4.0mm

7.5mm mpaka 10mm - 5.0mm

9.0mm mpaka 12mm - 6.0mm