Nkhani
-
Udindo wa Nickel Alloy Stick Welding Electrodes
Ma Electrode Omwe Amawotchera Ndodo a Nickel Alloy amapangidwira malo ovuta, okhala ndi kukana dzimbiri komanso kutentha kwambiri, ndipo ndi oyenera kugwiritsa ntchito mankhwala, mphamvu ndi ndege. Mphamvu zake zosiyanasiyana zowotcherera zitsulo komanso mawonekedwe ake okhazikika a arc zimatha kukwaniritsa...Werengani zambiri -
Ubwino wa E71T-8-H8 mu Kuwotcherera Chitsulo cha Carbon
E71T-8-H8 Yodziteteza Yokha ndi chinthu chowotcherera chapamwamba kwambiri chomwe chapangidwira makamaka kuwotcherera chitsulo cha kaboni ndi chitsulo chopanda aloyi. Sichifuna mpweya woteteza kunja ndipo ndi choyenera kwambiri pa ntchito zakunja komanso zachilengedwe zovuta. Ili ndi kutentha kochepa kwa -40℃...Werengani zambiri -
Kugwiritsa ntchito ndi kugwiritsa ntchito njira zoyeretsera waya
Waya Wowetsera ndi chinthu chowetsera chapamwamba kwambiri chomwe chimapangidwira kuwotcherera koyima, kuwotcherera kokhazikika paipi ndi malo ena ovuta, omwe amagwirizana ndi miyezo ya ASME 5G/6G. Ili ndi kukhazikika kwabwino kwambiri kwa arc komanso mawonekedwe otsika a spatter, kuonetsetsa kuti kuwotcherera kumakhala kogwirizana mbali zonse, ndipo...Werengani zambiri -
Za zotsatira ndi ntchito za zinthu za Electrode
Zogulitsa zama electrode ndi zinthu zofunika kwambiri pakuchita bwino kwa ma electrochemical ndi mayankho a mphamvu, ndipo zimagwiritsidwa ntchito kwambiri posungira mphamvu (monga mabatire, ma supercapacitor), zida zachipatala (kuwunika kwa ECG/EEG) ndi kuyang'anira chilengedwe (kusanthula khalidwe la madzi, kuzindikira kuipitsidwa). Ndi...Werengani zambiri -
Za ntchito ya E310-15 Welding Rod
Ndodo Yothira Ma waya ya E310-15 idapangidwa kuti igwiritsidwe ntchito pothira waya wothira kutentha kwambiri komanso wosagwirizana ndi dzimbiri, ndipo ndi yoyenera kulumikiza chitsulo chosapanga dzimbiri cha austenitic ndi zitsulo zosiyana (monga chitsulo chosapanga dzimbiri ndi chitsulo cha carbon). Kuchuluka kwa chromium ndi nickel kumapereka kukana kwabwino kwa okosijeni, kutentha kwambiri...Werengani zambiri -
Electrode Yowotcherera ya Carbon Steel Yogwira Ntchito Kwambiri Yowotcherera Malo Onse
Choyeretsera cha J421 (AWS E6013) Carbon Steel Welding Electrode chili ndi utoto wa potaziyamu kuti chitsimikizire kuti arc yosalala komanso yokhazikika komanso yopanda madzi ambiri. Kapangidwe kake kosinthasintha kamathandizira kuwotcherera kulikonse pogwiritsa ntchito magetsi a AC ndi DC, zomwe zimapangitsa kuti ikhale yoyenera kwambiri popanga ndi kukonza zinthu zonse. J4...Werengani zambiri -
Ndodo Yowotcherera ya Chitsulo Chosapanga Dzimbiri cha AWS E2209-16 Yapamwamba Kwambiri
AF2209-16 (AWS E2209-16) ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi calcium-titanium, yokhala ndi nayitrogeni, yokhala ndi carbon yochepa kwambiri. Ndodo Yothira Zitsulo Zosapanga Dzimbiri ya AWS E2209-16 idapangidwa kuti igwiritsidwe ntchito kwambiri pothira zingwe kuti zitsimikizire kuti malo olumikizirana ndi zingwe ndi olimba komanso osakhudzidwa ndi dzimbiri m'malo ovuta. ...Werengani zambiri -
Electrode Yothira Kaboni Imapangitsa Kuti Ntchito Zamakampani Ziziyenda Bwino
AWS E7024 Carbon Steel Welding Electrode (501Fe18) ndi electrode yachitsulo yopangidwa bwino kwambiri ya titanium alloy yopangidwa kuti igwiritsidwe ntchito mwachangu. Ndi yoyenera kulowetsedwa molunjika/molunjika ndipo imatha kupanga arc yosalala yokhala ndi kuyeretsa kochepa kwa slag pambuyo poweredwa. AWS A5.1 E7024 Carbon Steel Weld...Werengani zambiri -
Waya Wowotcherera wa AWS A5.7 ERCuSn-C Waya Wapamwamba Kwambiri Wowotcherera wa Copper Alloy
Waya Wowetsera wa Copper Alloy wa AWS A5.7 ERCuSn-C wapangidwa kuti ugwirizane ndi zitsulo zamkuwa ndi zamkuwa. Kukana kuyenda bwino kwa madzi ndi ming'alu kumatsimikizira kuti zitsulozo zimakhala zokhazikika nthawi yayitali, zomwe zimapangitsa kuti zikhale chisankho chabwino kwambiri pa ntchito zamagalimoto, zam'madzi ndi zamafakitale. Waya Wowetsera wa Copper Alloy wa AWS A5.7 ERCuSn-C ndi wabwino kwambiri...Werengani zambiri -
Waya Wowotcherera wa ENiFe-Cl Nickel Alloy Mig Wogwira Ntchito Kwambiri
Waya Wothira Mig Wothira Mig Wothira Mig Wothira Mig uli ndi mphamvu zabwino kwambiri zokonzera chitsulo chosungunuka ndi chitsulo chosungunuka. Kapangidwe kake kotsika kamatsimikizira kukhazikika kwa arc, komwe ndi koyenera kugwiritsidwa ntchito m'magalimoto, m'mafakitale komanso m'makina olemera. Waya Wothira Mig ...Werengani zambiri -
Ma Electrode a E316-16: Kuwotcherera kwa Chitsulo Chosapanga Zitsulo Zosapanga Zitsulo Zogwiritsidwa Ntchito Pamalo Ovuta
Ma Electrode a AWS E316-16 amagwiritsa ntchito titanium calcium coating, low carbon Cr18Ni12Mo2 alloy electrode, yoyenera kuwotcherera chitsulo chosapanga dzimbiri cha 316/316L. Ma Electrode a AWS E316-16 ali ndi arc yokhazikika komanso mpweya wochepa wa carbide, ndipo amagwira ntchito bwino pakugwiritsa ntchito mankhwala, madzi a m'nyanja komanso kutentha kwambiri. ...Werengani zambiri -
Waya Wolimba wa AWS A5.23 ECM4 Wamphamvu Kwambiri
Waya Wolimba wa AWS A5.23 ECM4 Wothira Madzi ndi ma electrode ochepa ophatikizika omwe amagwiritsidwa ntchito pothira madzi mwamphamvu kwambiri. Umakwaniritsa miyezo ya AWS A5.23 M4, kuonetsetsa kuti mphamvu yogwira ntchito ndi yoposa 110 ksi, kusunga kukhazikika kwa arc komanso kulimba kwa weld. Waya Wolimba wa AWS A5.23 ECM4 Wothira Madzi ndi ...Werengani zambiri