Kuwotcherera aluminiyamuNdi njira yofunika kwambiri m'mafakitale osiyanasiyana, makamaka polumikiza zinthu za aluminiyamu-magnesium zomwe zimafuna mphamvu zambiri zokoka. Chimodzi mwa zigawo zofunika kwambiri pakulumikiza aluminiyamu ndi waya wolumikizira, ndipo ER5183 ndi njira yotchuka yolumikizira MIG ya aluminiyamu-magnesium.
ER5183 yapangidwira makamaka kuwotcherera aluminiyamu-magnesium alloys zomwe zimafuna mphamvu yayikulu yokoka, makamaka pamene zinthu zoyambira ndi 5083 kapena 5654. Waya wowotcherera uwu umagwiritsidwa ntchito kwambiri m'zombo, nsanja za m'mphepete mwa nyanja, sitima zapamadzi, magalimoto, magalimoto, makontena, zotengera za cryogenic, ndi zina zotero.
ER5183 imapereka zabwino zingapo polumikiza zitsulo za aluminiyamu ndi magnesium. Mphamvu zake zolimba kwambiri zimapangitsa kuti ikhale yoyenera kugwiritsidwa ntchito pomwe kulimba kwa kapangidwe kake ndikofunikira. Kuphatikiza apo, ER5183 imadziwika kuti imakana dzimbiri, zomwe zimapangitsa kuti ikhale yoyenera kwambiri pazinyumba zolumikizidwa zomwe zili ndi nyengo yovuta, monga malo am'madzi kapena m'mphepete mwa nyanja.
Kuphatikiza apo, waya wowotcherera wa ER5183 umadziwika chifukwa cha kusinthasintha kwake bwino komanso kusinthasintha pang'ono kwa kutentha, zomwe zimapangitsa kuti njira yowotcherera ikhale yosalala komanso yodalirika. Kusinthasintha kwake komanso kuthekera kwake kopanga ma weld apamwamba kumapangitsa kuti ikhale chisankho choyamba cha opanga ndi owutchulira omwe amagwira ntchito ndi aluminiyamu-magnesium alloys.
Mwachidule, waya wowotcherera wa aluminiyamu wa ER5183 ndiye njira yoyamba yowotcherera wa MIG wa aluminiyamu-magnesium alloys omwe amafunikira mphamvu yayikulu yolimba komanso kukana dzimbiri. Ntchito zake zimayambira pakupanga zombo mpaka kupanga magalimoto, zomwe zimapangitsa kuti ikhale chida chofunikira kwambiri kwa opanga ndi owutchulira. Ndi mphamvu zake zapamwamba komanso kudalirika kwake, ER5183 ndiye yankho labwino kwambiri la kuwotcherera kwamphamvu komanso kolimba m'mapangidwe a aluminiyamu-magnesium alloy.
Nthawi yotumizira: Juni-11-2024