Kodi Ndodo Yotani Yowetsera Imagwiritsidwa Ntchito Pa Chitsulo cha Carbon?

Pa ntchito iliyonse yachitsulo cha kaboni, kaya kukonza, kupanga, kapena ntchito ya mapaipi, kusankha ndodo yoyenera yowotcherera ndikofunikira kwambiri pa chowotcherera champhamvu komanso cholimba. Ndiye, ndi ndodo iti yowotcherera yomwe imagwiritsidwa ntchito pachitsulo cha kaboni? Ngakhale kuti mndandanda wa E6010, E6011, E7018, ndi E7024 ndi zosankha zofala komanso zosinthika, njira yabwino kwambiri imadalira zosowa zanu. Kumvetsetsa zosiyanaMpweya Wowotcherera wa Chitsulo cha CarbonMitundu idzakuthandizani kufananiza ndodo ndi gwero lanu lamagetsi, malo olumikizirana, ndi zofunikira pa ntchito.'fufuzani ma electrode otchuka, momwe amagwiritsidwira ntchito, ndi momwe mungasankhire moyenera.

Kumvetsetsa Ma Electrode Othandizira Kuwedza Kaboni

Electrode Yothira Mpweya wa Carbon Steel ndi waya wachitsulo wophimbidwa ndi flux. flux imalimbitsa arc, imateteza weld yosungunuka ku kuipitsidwa ndi mpweya, ndipo imatha kuphatikiza ma alloy kuti iwonjezere mphamvu za weld. Electrode imatsatira njira yodziwika bwino yowerengera yomwe imasonyeza mphamvu zawo zomangika, malo oyenera owetera, mtundu wa flux, ndi mphamvu yogwirizana.

Mitundu Yotchuka ya Electrode ya Chitsulo cha Carbon

1. E6010 ndi E6011

  • Zinthu Zofunika Kwambiri: Izi ndi ma electrode opangidwa ndi cellulose, omwe amaundana mwachangu. Amapanga arc yozama, yolowera bwino kwambiri yolumikizira mizu pa mapaipi kapena malo olumikizirana okhala ndi mipata.
  • Mphamvu: E6010 imagwira ntchito pa DC+ yokha. E6011 ndi yosinthasintha kwambiri ndipo imatha kugwira ntchito pa AC ndi DC.
  • Zabwino Kwambiri: Kuwotcherera mapaipi, kuwotcherera pansi, ndi kukonza zinthu zonse zomwe zimalowa mkati. Zotsalira zake zimakhala zopyapyala ndipo zimachotsedwa mosavuta.

2. E7018

  • Zinthu Zofunika Kwambiri: Kawirikawiri imatchedwa "low-hydrogen" kapena "stick electrode," iyi ndi njira yogwirira ntchito ya chitsulo chomangira. Ili ndi arc yosalala komanso yokhazikika yokhala ndi ufa wachitsulo mu flux, zomwe zimawonjezera kuchuluka kwa ma depositi.
  • Mphamvu: Imagwira ntchito pa AC kapena DC+ (DC imakonda).
  • Zabwino Kwambiri: Zosefera zofunika kwambiri zomwe zimafuna mphamvu zambiri komanso kukana kugwedezeka bwino. Zimapanga zosefera zabwino kwambiri m'malo onse ndipo zimadziwika ndi mawonekedwe ake abwino kwambiri a mikanda komanso kukana ming'alu.

3. E7024 ndi E7014

  • Zinthu Zofunika Kwambiri: Izi ndi ma electrode a ufa wachitsulo omwe amathiridwa kwambiri, okhala ndi madzi ambiri. Amapanga mzere wosalala wokhala ndi madzi ochepa komanso matope olemera omwe amatuluka mosavuta.
  • Mphamvu yamagetsi: AC kapena DC.
  • Zabwino Kwambiri: Fillet yothamanga kwambiri, yathyathyathya kapena yopingasa imasweda pomwe mawonekedwe ndi liwiro loyenda ndizofunikira.

Momwe Mungasankhire Ndodo Yoyenera: Buku Losavuta

KusankhaKuwotcherera kwa Chitsulo cha Kaboni kolondolaElectrode imaphatikizapo kuyang'ana tsatanetsatane wa polojekitiyi:

1.Chongani Mphamvu ya Chitsulo Choyambira: Gwirizanitsani mphamvu ya electrode (manambala awiri oyamba pambuyo pa 'E') ndi chitsulo chanu. Pa chitsulo chodziwika bwino cha A36 (36,000 psi yield), ndodo ya mndandanda wa E60xx kapena E70xx ndiyoyenera.

2.Dziwani Malo Omwe Muli Kuwotcherera: Nambala yachitatu imasonyeza malo omwe muli.

  • 1 = Malo Onse (E7018)
  • 2 = Malo athyathyathya ndi opingasa okha (E7024)

3.Dziwani Gwero Lanu la Mphamvu: Onetsetsani kuti chowotcherera chanu (AC, DC+, DC-) chikupereka mtundu wamagetsi womwe electrode imafuna.

4.Ganizirani Kapangidwe ndi Mkhalidwe wa Ma Joint: Gwiritsani ntchito ndodo zolowera mozama (E6010) kuti mupeze mipata kapena mizu yodutsa. Gwiritsani ntchito ndodo zopanda hydrogen wambiri (E7018) kuti mupeze zigawo zokhuthala kapena malo olumikizirana kuti mupewe ming'alu.

Njira Zabwino Kwambiri Zothandizira Kuwotcherera Moyenera

Sungani Ndodo Moyenera: Ndodo zopanda haidrojeni wambiri zimakhudzidwa ndi chinyezi. Zisungeni mu uvuni wotsekedwa, makamaka m'malo ozizira, kuti mupewe kusweka ndi kusweka chifukwa cha haidrojeni.

Tsukani Chitsulo Choyambira: Nthawi zonse chotsani dzimbiri, mafuta, utoto, ndi sikelo ya mphero pamalo olumikizirana kuti mugwiritse ntchito weld yoyera kwambiri.

Tsatirani Ma Parameter a Wopanga: Gwiritsani ntchito amperage range yovomerezeka ndi liwiro loyendera pa datasheet ya electrode.

Kupeza Ma Electrode Odalirika Othandizira Kuwetsa

Kwa osonkha, opanga zinthu, kapena oyang'anira kugula, kusinthasintha ndi khalidwe sizingakambirane. Ma electrode oipa angayambitse kulephera kwa weld, kukonzanso, komanso nthawi yotsika mtengo yopuma. Pogula zinthu za Carbon Steel Welding Electrode, akatswiri ambiri amafunafuna ogulitsa omwe amaphatikiza magwiridwe antchito odalirika ndi maubwino othandiza a unyolo woperekera zinthu.

Opanga monga Tianyu Electronic apanga mizere yawo yazinthu kuti akwaniritse izi, ndikupanga ma electrode omwe akutsatira miyezo yapadziko lonse lapansi. Kwa mabizinesi omwe akuchita mapulojekiti akuluakulu, kupanga, kapena kukonza, kupezeka kwa mitengo yokwera kungapangitse kusiyana kwakukulu pakukonza bajeti ya polojekiti. Kugwirizana ndi wogulitsa yemwe amasunga netiweki yogawa padziko lonse lapansi kumathandiza kuonetsetsa kuti kutumiza ndi chithandizo chaukadaulo kuperekedwa panthawi yake, pomwe mitundu yonse yazinthu imalola kupeza mitundu yosiyanasiyana ya ma electrode kuchokera kwa mnzanu m'modzi wodalirika.

Malangizo Omaliza

Kodi ndodo yabwino kwambiri yolumikizira zitsulo za kaboni ndi iti? Kuti mupeze ma weld amphamvu kwambiri komanso osinthasintha, sungani ma electrode a E7018 m'sitolo yanu, pomwe ndodo za E6010/E6011 ndizoyenera kugwiritsa ntchito mapaipi apadera kapena kulowa mozama. Nthawi zonse onani zofunikira za polojekiti yanu kapena njira yolumikizira poyamba. Kumbukirani, kuwotcherera kopambana kumadalira ma electrode abwino, kusungirako koyenera, komanso njira yabwino. Pomvetsetsa izi zomwe zimafala kwambiri.Mpweya Wowotcherera wa Chitsulo cha Carbonmitundu ndi kagwiritsidwe ntchito kake, mutha kuthana ndi ntchito iliyonse yachitsulo cha kaboni molimba mtima, kuonetsetsa kuti zotsatira zake ndi zolimba, zokhazikika, komanso zotsatizana ndi malamulo nthawi iliyonse.