AW DURMATIC (H-10) Electrode Yowetsera Yolimba, Ndodo Yowetsera Yowonekera Pamwamba, Ndodo Yowetsera Yozungulira

Kufotokozera Kwachidule:

Ma electrode ophikira olimba pa zitsulo zatsopano kapena zakale, chitsulo cha manganese kapena chitsulo chofewa. Zigawo kapena zigawo zake zimakhala ndi kukwawa kwambiri.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Hardfacing Welding Stick Electrode

AW DURMATIC H-10

Kuzindikira malo: ORANGE

KUFOTOKOZA:

Ma electrode ophikira olimba pa zitsulo zatsopano kapena zosweka, chitsulo cha manganese kapena chitsulo chofewa. Mu zigawo kapena zigawo zomwe zimakhudzidwa kwambiri. Gwiritsani ntchito electrode direct current (CDPI), yomwe imakhala ndi kuuma kwakukulu kuchokera ku bead yoyamba, imathandizira magawo atatu osavuta kugwiritsa ntchito chifukwa cha maziko ake a austenitic ndi arc yofewa. Ma chromium carbides, mikanda yowoneka bwino komanso yosavuta kuchotsa slag.

NTCHITO:

Chogulitsachi n'chosavuta kugwiritsa ntchito ndipo chimagwiritsidwa ntchito mumakampani omanga, poponda ndi kusuntha makina a nthaka ndi miyala, kuti apezenso, ateteze ndikupatsa zida zamtunduwu moyo wautali.

Mu mafakitale ambiri, ndi yoyenera pazochitika zambiri zogwiritsidwa ntchito powonongeka chifukwa cha kusweka kwakukulu komanso kukhudzidwa pang'ono, mwachitsanzo: zosakaniza mchenga kapena zinthu zokwawa, zotsetsereka, makamera, shafts, zodulira, zodulira, mphero ndi zida zotulutsira, ndi zina zotero.

Amagwiritsidwa ntchito ngati gawo lomaliza pa zokutira zina kapena matiresi olumikizirana.

UBWINO:

Mwa gulu la ma electrode okutira kuti awonongeke kwambiri, ndi omwe ali ndi ntchito yosavuta kugwiritsa ntchito, kuchotsa slag ndi kukhazikika kwa arc, kuuma kwake kwakukulu kumachitika chifukwa chakuti ali ndi maziko a chromium carbide, okana kwambiri kuvala, chifukwa cha kusweka kwambiri komanso kugunda kwapakati. . Malo osalala okhala ndi mapeto abwino, opanda ma pores komanso osavuta kuchotsa slag; Alloy iyi imalimbikitsidwa pamene sizingatheke kuyika mikanda yoposa itatu yokutira chifukwa ili ndi kusungunuka kochepa kwambiri ndi chitsulo choyambira, motero imapangitsa kuti mkanda woyamba ukhale wolimba kwambiri.

 

Katundu Wamba wa Makina a Chitsulo Chosungidwa

m'mimba mwake wa elekitirodi 3.2mm(1/8)") 4.0mm(5/32") 4.8mm(3/16")
Kuuma 56HRC 56.8HRC 55.7HRC

 

Kapangidwe ka OUMIC ka Chitsulo Chosungidwa

 

Silikoni          1.34%

Manganese      1.09%

Mpweya         2.63%

Chrome        30.99%

Sulfure         0.03%

Molybdenum    0.06%

 

NJIRA YOWOTEZERA

Musanagwiritse ntchito alloy, onetsetsani kuti chidutswa chomwe mukufuna kuchipaka chilibe ma oxides, mafuta kapena zigawo zachitsulo chotopa, ndi zina zotero. Pamene pamwamba pa chitsulo choyambira chayera, pitirizani kuyika mikanda yowongoka kapena mwanjira yoti kugwedezeka kwa electrode kusapitirire katatu kuposa kukula kwake. Tsukani zinyalala pakati pa ma pass; mukamaliza lolani chidutswacho kuti chizire pang'onopang'ono.

 

NJIRA ZOMWE ZILIPO

mm

mainchesi

Ampere

3.2 X 356

1/8 X 14

100-140

4.0 X 356

5/32 X 14

130-180

4.8 X 356

3/16 X 14

170-210

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu ndi chitsulo chosapanga dzimbirielekitirodi yowotchereras, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo za low alloy, ma electrode olumikizira zitsulo za surfacing, ma electrode olumikizira zitsulo za nickel & cobalt alloy, mawaya olumikizira zitsulo zopepuka & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira aluminiyamu, mawaya olumikizira zitsulo za arc. mawaya, mawaya olumikizira zitsulo za nickel & cobalt alloy, mawaya olumikizira zitsulo zamkuwa, mawaya olumikizira zitsulo za TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo za kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 

 

 

 