Nickel Alloy Welding Waya ERNiCrMo-3 Tig Waya

Kufotokozera Kwachidule:

ERNiCrMo-3 ndi waya wapamwamba wa nickel alloy wopangidwira kuwotcherera ndi kuyika ma alloys opangidwa ndi nickel monga 625 kapena zinthu zina zofananira.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Nickel AlloyWaya WowotchereraTig WayaERNiCrMo-3

 

Features ndi Mapulogalamu

Wapamwambanickelwaya wa alloy wopangidwira kuwotcherera ndi kuwotchereranickel-aloyi zoyambira monga 625 kapena zinthu zofananira.

Zolimba zomwe zimakokedwa mwanjira yapadera kwambiri kuti mupeze ma welds oyeretsera komanso apamwamba kwambiri okhala ndi msoko wowala komanso ductility wabwino kwambiri.

Chitsulo chowotcherera chimakhala ndi makina abwino kwambiri pamatenthedwe apamwamba komanso otsika.

Kukaniza bwino kwa pitting ndi kupsinjika kwa dzimbiri.

Kutentha kovomerezeka kogwirira ntchito kumayambira pa cryogenic mpaka 540°C.

Amagwiritsidwa ntchito pamakampani opanga mankhwala, mainjiniya apanyanja, zida zanyukiliya, zakuthambo komanso zida zowongolera kuipitsidwa ndi zina.

Zida Zomwe Zimayambira

Inconel 601, Aloyi 800, Aloyi 625, Aloyi 825, Aloyi 926*
* Mndandanda wazithunzi, osati wokwanira

 

Miyezo
EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb
AWS A5.14 – ER NiCrMo-3

 

Chemical Composition%

C%

Mn%

Fe%

P%

S%

Si%

Ku%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ndi%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

min

1.0

0.40

0.40

23.00

4.15

10.00

 

Mechanical Properties
Kulimba kwamakokedwe ≥760 MPa  
Zokolola Mphamvu ≥415 MPa  
Elongation ≥35%  
Mphamvu Zamphamvu ≥100 J  

Makina amakina ndi oyerekeza ndipo amatha kusiyanasiyana kutengera kutentha, kutchingira mpweya, zowotcherera ndi zina.

 

Kuteteza Magesi

TS EN ISO 14175 TIG: I1 (Argon)

 

Malo Owotcherera

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Packaging Data
Diameter Utali Kulemera  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

 

Udindo: Ngakhale zoyesayesa zonse zakhala zikuchitika kuti zitsimikizire kulondola kwa zomwe zili, chidziwitsochi chikhoza kusintha popanda chidziwitso ndipo chitha kuonedwa ngati choyenera kuwongolera wamba.

 


  • Zam'mbuyo:
  • Ena: