Waya Wowotcherera wa Nickel Alloy ERNiCrMo-3 Mig Welding Waya

Kufotokozera Kwachidule:

ERNiCrMo-3 ndi waya wapamwamba wa nickel alloy wopangidwira kuwotcherera ndi kuyika ma alloys opangidwa ndi nickel monga 625 kapena zinthu zina zofananira.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Nickel AlloyWaya WowotchereraERNiCrMo-3

 

Miyezo

EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb

AWS A5.14 – ER NiCrMo-3

 

Features ndi Mapulogalamu

Wapamwambanickelwaya wa alloy wopangidwira kuwotcherera ndi kuwotchereranickel-aloyi zoyambira monga 625 kapena zinthu zofananira.

Zolimba zomwe zimakokedwa mwanjira yapadera kwambiri kuti mupeze ma welds oyeretsera komanso apamwamba kwambiri okhala ndi msoko wowala komanso ductility wabwino kwambiri.

Chitsulo chowotcherera chimakhala ndi makina abwino kwambiri pamatenthedwe apamwamba komanso otsika.

Kukaniza bwino kwa pitting ndi kupsinjika kwa dzimbiri.

Kutentha kovomerezeka kogwirira ntchito kumayambira pa cryogenic mpaka 540°C.

Mwatsatanetsatane wosanjikiza bala kwa apamwamba mawaya kudyetsa makhalidwe.

Amagwiritsidwa ntchito pamakampani opanga mankhwala, mainjiniya apanyanja, zida zanyukiliya, zakuthambo komanso zida zowongolera kuipitsidwa ndi zina.

 

Zida Zomwe Zimayambira

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926* * Mndandanda, osati wokwanira

 

Chemical Composition%

C%

Mn%

Fe%

P%

S%

Si%

Ku%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ndi%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

Min

1.0

0.40

0.40

23.00

4.15

10.00

 

Mechanical Properties

Kulimba kwamakokedwe

≥760 MPa

Zokolola Mphamvu

≥415 MPa

Elongation

≥35%

Mphamvu Zamphamvu

≥100 J

Makina amakina ndi oyerekeza ndipo amatha kusiyanasiyana kutengera kutentha, kutchingira mpweya, zowotcherera ndi zina.

Kuteteza Magesi

TS EN ISO 14175 - I1, I3

Malo Owotcherera

TS EN ISO 6947 PA, PB, PC, PD, PE, PF

Packaging Data

Diameter

Kulemera

Spool

Pallet Qty

1.00 mm

1.20 mm

15 Kg

15 Kg

BS300

BS300

72

72