Waya Wowotcherera wa Chitsulo Chosapanga Dzimbiri wa Flux Cored Waya wa E316LT-1

Kufotokozera Kwachidule:

E316LT-1 imagwiritsidwa ntchito kwambiri pa zitsulo zoyambira zopangidwa mofanana monga AISI Types 301, 302, 304, 305 ndi 308. Kuchuluka kwa kaboni kokwanira 0.04% kumalola kukana kwambiri dzimbiri la pakati pa granular komanso kuchepetsa mvula ya carbide.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Chitsulo chosapanga dzimbiriFlux CoredWaya E316LT-1

MAWU OYAMBA
E316LT-1 imagwiritsidwa ntchito kwambiri pa zitsulo zoyambira zomwe zili ndi zinthu zofanana monga AISI Types 301, 302, 304, 305 ndi 308. Kuchuluka kwa kaboni kokwanira 0.04% kumalola kukana kwambiri dzimbiri la pakati pa granular komanso kuchepetsa mvula ya carbide. Mawaya awa apangidwa kuti agwiritsidwe ntchito ndi 100% CO2 kapena 80% Ar/20% CO2 shielding gas. Kutha kugwira ntchito pamitundu yosiyanasiyana yamagetsi kumalola kuchuluka kwa ma deposition omwe ndi okulirapo nthawi 4 kuposa ma electrode ophimbidwa komanso mpaka 50% kuposa waya wolimba wa MIG. Ngakhale mtengo pa paundi ya mawaya a Stainless Steel Flux-Cored ukhoza kukhala woposa wa ma electrode ophimbidwa kapena waya wolimba wa MIG, mtengo wanu pa paundi ya chitsulo chosungunuka chosungidwa umachepa kwambiri chifukwa cha kuchuluka kwa ma deposition komanso ndalama zochepa zogwirira ntchito. Chigoba chenicheni chachitsulo chosapanga dzimbiri chomwe chimagwiritsidwa ntchito popanga Aufhauser Flux-Cored Stainless ndi chitsimikizo chanu cha magwiridwe antchito osalala, ma welds abwino a x-ray komanso mawonekedwe okongola a bead achitsulo chosapanga dzimbiri. Kuthira kwa madzi ndi kochepa kwambiri ndipo matope amadzichotsa okha.

NTCHITO
Kuwotcherera ma alloys ofanana omwe ali ndi pafupifupi 2% molybdenum
Kugwiritsa ntchito kutentha (molybdenum imawonjezera kukana kwa kukwawa pa kutentha kwakukulu)

ZINA ZAMBIRI
Kapangidwe ka Mankhwala

Mpweya Chromium Fakitoli Molybdenum Manganese Silikoni Phosphorus Sulfure Mkuwa Chitsulo
0.04 17.0-20.0 11.0-14.0 2.0-3.0 0.5-2.5 1.0 0.04 0.03 0.5 Rem

Katundu Wathupi Ndi Wamakina

Kulimba kwamakokedwe 70,000 psi
Kuchulukana –
Kutalika, osachepera % 30

 

ZOTSATIRA ZIKUKWANIRA KAPENA KUPITA PAMENEPO
AWS: A5.22
ASME: SFA 5.22

 

Kukula Koyenera ndi Ma Diameter
Ma diameter: 0.035″, 0.045″, ndi 1/16″

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.