Kufotokozera Kwachidule:

E309LT-1 imagwiritsidwa ntchito kwambiri pa zitsulo zoyambira zopangidwa mofanana monga AISI Types 301, 302, 304, 305 ndi 308. Kuchuluka kwa kaboni kokwanira 0.04% kumalola kukana kwambiri dzimbiri la pakati pa granular komanso kuchepetsa mvula ya carbide.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Chitsulo chosapanga dzimbiriFlux CoredWaya E309LT-1

MAWU OYAMBA
E309LT-1 imagwiritsidwa ntchito kwambiri pa zitsulo zoyambira zomwe zili ndi zinthu zofanana monga AISI Types 301, 302, 304, 305 ndi 308. Kuchuluka kwa kaboni kokwanira 0.04% kumalola kukana kwambiri dzimbiri la intergranular komanso kuchepetsa mvula ya carbide. Mawaya awa apangidwa kuti agwiritsidwe ntchito ndi 100% CO2 kapena 80% Ar/20% CO2 shielding gas. Kutha kugwira ntchito pamitundu yosiyanasiyana yamagetsi kumalola kuchuluka kwa ma deposition omwe ndi ochulukirapo nthawi 4 kuposa ma electrode ophimbidwa komanso mpaka 50% kuposa waya wolimba wa MIG. Ngakhale mtengo pa paundi ya mawaya a Stainless Steel Flux-Cored ukhoza kukhala woposa wa ma electrode ophimbidwa kapena waya wolimba wa MIG, mtengo wanu pa paundi ya chitsulo chosungunuka chosungidwa umachepa kwambiri chifukwa cha kuchuluka kwa ma deposition komanso ndalama zochepa zogwirira ntchito. Chigoba chenicheni chachitsulo chosapanga dzimbiri chomwe chimagwiritsidwa ntchito popanga Aufhauser Flux-Cored Stainless ndi chitsimikizo chanu cha magwiridwe antchito osalala, ma welds abwino a x-ray komanso mawonekedwe okongola a bead achitsulo chosapanga dzimbiri. Kuthira kwa madzi ndi kochepa kwambiri ndipo matope amadzichotsa okha.

NTCHITO
Kulukana zitsulo zofanana mu mawonekedwe opangidwa kapena opangidwa ndi chitsulo
Kuwotcherera zitsulo zosiyana, monga: kulumikiza Mtundu 304 ku chitsulo chofewa, kuwotcherera mbali ya chitsulo chosapanga dzimbiri ya zitsulo zophimbidwa ndi Mtundu 304, ndikugwiritsa ntchito mapepala achitsulo chosapanga dzimbiri pa mapepala achitsulo cha kaboni
Nthawi zina amagwiritsidwa ntchito powotcherera zitsulo zamtundu wa 304 m'mikhalidwe yoopsa ya dzimbiri
Imagwiritsidwa ntchito popangira chitsulo cha kaboni ngati palibe chowonjezera cha columbium chomwe chikufunika.

ZINA ZAMBIRI
Kapangidwe ka Mankhwala

Mpweya Chromium Fakitoli Molybdenum Manganese Silikoni Phosphorus Sulfure Mkuwa Chitsulo
0.04 22.0-25.0 12.0-14.0 0.5 0.5-2.5 1.0 0.04 0.03 0.5 Rem

Katundu Wathupi Ndi Wamakina

Kulimba kwamakokedwe 75,000 psi
Kuchulukana –
Kutalika, osachepera % 30

 

ZOTSATIRA ZIKUKWANIRA KAPENA KUPITA PAMENEPO
AWS: A5.22
ASME: SFA 5.22

 

Kukula Koyenera ndi Ma Diameter
Ma diameter: 0.035″, 0.045″, ndi 1/16″

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.