AWS A5.4 E309Mo-15 Electrode Yopanda Chitsulo Chosapanga Dzimbiri Yokhala ndi Chophimba Chochepa cha Hydrogen Sodium, Ndodo Zowetsera

Kufotokozera Kwachidule:

A317 (AWS E309Mo-15) ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi chofunda chochepa cha hydrogen sodium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi

A317                                     

GB/T E309Mo-15

AWS A5.4 E309Mo-15

Kufotokozera: A317 ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi hydrogen sodium yochepa. Gwiritsani ntchito DCEP (electrode yamagetsi yolunjika). Ili ndi kukana dzimbiri, ming'alu, komanso okosijeni kuposa A302 chifukwa chitsulo chosungidwacho chili ndi molybdenum.

Kugwiritsa Ntchito: Amagwiritsidwa ntchito polukira chitsulo chosapanga dzimbiri, mbale yachitsulo yophatikizika ndi chitsulo chosiyana chomwe chimalimbana ndi dzimbiri la sulfuric acid (sulfur ammonia).

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥550

≥25

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.0

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Zindikirani:

Elektrodi iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 250℃ isanayambe kuwotcherera.

 

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.

Zogulitsa zathu zazikulu ndi chitsulo chosapanga dzimbirielekitirodi yowotchereras, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo za low alloy, ma electrode olumikizira zitsulo za surfacing, ma electrode olumikizira zitsulo za nickel & cobalt alloy, mawaya olumikizira zitsulo zopepuka & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira aluminiyamu, mawaya olumikizira zitsulo za arc. mawaya, mawaya olumikizira zitsulo za nickel & cobalt alloy, mawaya olumikizira zitsulo zamkuwa, mawaya olumikizira zitsulo za TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo za kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 