AWS E317-16 Zitsulo Zosapanga Zitsulo Zosenda Zozungulira ...

Kufotokozera Kwachidule:

A242 (AWS E317-16) ndi electrode yachitsulo chosapanga dzimbiri ya Cr19Ni13Mo3 yopanda kaboni wambiri yokhala ndi zokutira za titanium-calcium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi

A242                                      

GB/T E317-16

AWS A5.4 E317-16

Kufotokozera: A242 ndi electrode yachitsulo chosapanga dzimbiri ya Cr19Ni13Mo3 yopanda kaboni yokhala ndi zokutira za titanium-calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri. Chitsulo chosungidwacho chili ndi kuchuluka kwa molybdenum kuposa A202, ndipo chimakhala ndi kukana dzimbiri kwa ma asidi osapanga okosijeni, monga sulfuric acid, sulfurous acid, phosphoric acid ndi organic acids. Imakhalanso ndi mphamvu yabwino yolimbana ndi dzimbiri.

Kugwiritsa Ntchito: Kugwiritsidwa ntchito polumikiza zinthu zachitsulo chosapanga dzimbiri zomwezo komanso chitsulo chosakanikirana ndi chitsulo chosiyana.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥550

≥25

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa 150℃ isanayambe kuwotcherera;

2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yolumikiza magetsi a AC, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse.

 

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 