AWS: SFA 5.4 E316-16 Ma Electrode Osenda a Chitsulo Chosapanga Dzimbiri

Kufotokozera Kwachidule:

A201(AWS E316-16) ndi electrode yachitsulo chosapanga dzimbiri ya Cr18Ni12Mo2 yopanda kaboni wambiri yokhala ndi zokutira za titanium-calcium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Chitsulo chosapanga dzimbiri chowotcherera maelekitirodi

A201                                      

GB/T E316-16

AWS E316-16

Kufotokozera: A201 ndi electrode yachitsulo chosapanga dzimbiri ya Cr18Ni12Mo2 yopanda kaboni yokhala ndi zokutira za titanium-calcium. Ingagwiritsidwe ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri, makamaka yoyenera kuwotcherera molunjika komanso kuwotcherera minofu ya mbale zoonda. Chophimbacho sichimafiira kapena kusweka panthawi yowotcherera. Chifukwa cha kuwonjezera kwa molybdenum kuchitsulo chomwe chayikidwa, chimakhala ndi kukana dzimbiri, kukana kutentha komanso kukana ming'alu, makamaka polimbana ndi dzimbiri la chloride ion.

Kugwiritsa Ntchito: Kugwiritsidwa ntchito powotcherera zitsulo zosapanga dzimbiri za 06Cr17Ni12Mo2 zomwe zimagwira ntchito mu organic ndi inorganic acid (non-oxidizing acid), ndipo kungagwiritsidwenso ntchito kuwotcherera zitsulo zambiri za chromium kapena zitsulo zosiyana zomwe sizingathe kutenthedwa pambuyo powotcherera.

 

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥520

≥30

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.0

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha pafupifupi 250℃ musanagwiritse ntchito kuwotcherera. Musaphike mobwerezabwereza;

2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yolumikiza magetsi a AC, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri.

 

Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.


  • Yapitayi:
  • Ena: