AFE312-16 (AWS E312-16) ndi electrode yachitsulo chosapanga dzimbiri ya Cr29Ni9 yokhala ndi zokutira za titanium-calcium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Chitsulo chosapanga dzimbiri chowotcherera maelekitirodi

AF312-16

GB/T E312-16

AWS A5.4 E312-16

Kufotokozera: AFE312-16 ndi electrode yachitsulo chosapanga dzimbiri ya Cr29Ni9 yokhala ndi zokutira za titanium-calcium. Itha kugwiritsidwa ntchito pa AC ndi DC ndipo imagwira ntchito bwino kwambiri. Chifukwa ili ndi molybdenum ndi nayitrogeni, ndipo mpweya woipa ndi wochepa kwambiri, chitsulo chomwe chili mu chitsulocho chimakhala ndi kukana bwino ming'alu komanso dzimbiri, makamaka kukana dzimbiri.

Kugwiritsa Ntchito: Amagwiritsidwa ntchito polumikiza zitsulo zosapanga dzimbiri zamitundu 29-9, zitsulo zotayidwa ndi zitsulo zosiyana, komanso kulumikiza zinthu zomwe zimakhala ndi ming'alu komanso ma pores.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

28.0 ~ 32.0

8.0 ~ 10.5

≤0.75

≤0.75

≤0.030

≤0.040

 

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

 Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥660

≥22

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

()mm)

2.5

3.2

4.0

5.0

kuwotcherera Current

()A)

50 ~ 80

80 ~ 110

100 ~ 150

140 ~ 180

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha pafupifupi 250℃ isanayambe kuwotcherera.

 

Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 