Waya wa E2553T1-1/4 AP FLUX-CORED

KUGAŴA M'MAGWIRIZANO
AWS 5.22 Kalasi E2553T1-1 ndi E2553T1-4 / ASME SFA 5.22 Kalasi E2553T1-1 ndi E2553T1-4
UNS# W39533 A#8 F#6

KUFOTOKOZA
E2553T1-4 ndi waya wozungulira womwe umagwiritsidwa ntchito pa 75% Ar / 25% CO2.
Waya uwu wapangidwa kuti ukhale ndi njira yabwino kwambiri yochotsera matope ndipo umagwira ntchito popanda kufalitsa globular.

NTCHITO
Waya wopangidwa ndi flux-cored wa E2553T1-4 AP umagwiritsidwa ntchito polumikiza zitsulo zosapanga dzimbiri ziwiri zokhala ndi Chromium pafupifupi 25%.
Zitsulo zosapanga dzimbiri zimenezi zimaphatikiza mphamvu zokoka komanso zotulutsa mphamvu zambiri komanso kukana bwino ku dzenje, dzimbiri, komanso kusweka kwa dzimbiri. Zofunikira izi nthawi zambiri zimapezeka m'mafakitale a m'nyanja, mankhwala, ndi mafuta.
Ngati kulowetsedwa kwa chitsulo pambuyo pa weld kukufunika, chitsulo cholowetsedwachi chidzafunika kutentha kwakukulu kwa annealing kuposa komwe kumafunikira ndi chitsulo choyambira cha duplex.

NJIRA YOPHUNZITSIRA
Palibe kutentha koyambirira. Kutentha kwakukulu kwa interpass ndi 300°F.
Kuphimba pansi kungafunike kuti pakhale kuuma kofanana pa ma welds ambiri.
Kutentha kuyenera kukhala kochepera 5-40 KJ/IN.

KHEMISTIRI YACHIZINDIKIRO

C Cr Ni Mo Mn Si P S N Cu
0.02 25.3 9.8 3.37 0.80 0.70 0.03 0.015 0.14 1.87

KATUNDU WACHILENGEDWE WA MAKANIKO

KULIMA 25 RC monga cholukidwa 35 RC ntchito yolimba
KULIMBA KWAMAKOKEDWE 110,000 PSI Min.
KULEMERA 15% Osachepera.

MAGWARO OWOTCHERA

SIZE VOTEJI AMPERAGE GESI
.045” 25-30 130-220 75% Ar / 25% CO2 kapena 100% CO2

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.