E308L-17 Yopangira Ndodo Yowotcherera ya Electrode Yopanda Zitsulo Zosapanga Zitsulo (Low C, 18%Cr- 8%Ni)
Magulu
EN IS03581-A:2016: E 19 9 L R 12
EN IS03581-B:2016: ES308L-17
AWS A5.4-2014: E308L-17
JISZ 3221-2013: ES308L-17
Kufotokozera
-Chophimbacho ndi cha mtundu wa titania wa lime chomwe chimawotcherera chitsulo chosapanga dzimbiri cha 18%Cr-8%Ni. (AISI 301, 302, 304, 308)
-Kugwira bwino ntchito yowotcherera chifukwa cha kuchuluka kwa ma depositions.
-Chotsani madzi, dzimbiri, mafuta ndi zinthu zina zonse zakunja musanayambe kusonkha.
-Kugwiritsidwa ntchito bwino ndi mapulogalamu a direct current.
-Kutenthetsa sikofunikira nthawi zambiri.
-Tsambitsaninso electrode pa 250~350°C kwa mphindi 30~60 musanagwiritse ntchito.
| Kapangidwe ka Mankhwala Chitsulo Chosungidwa (%) | |||||||||
| C | Mn | Si | Cr | Ni | S | P | Mo | Cu | Fn |
| 0.03 | 0.65 | 0.73 | 18.95 | 9.82 | 0.012 | 0.028 | 0.21 | 0.30 | 6.4 |
| Kukula & Mphamvu Yoyenera (AC kapena DC) | ||||
| Kuwotcherera ndodo m'mimba mwake (mm) | 2.5 | 3.2 | 4.0 | 5.0 |
| kuwotcherera kwamakono (A) | 55-80 | 90-130 | 110-150 | 140-180 |
Makhalidwe Ogwiritsira Ntchito:
Mzere wokhazikika kwambiri.
Kuchotsa bwino kwambiri kwa slag.
Kulowa m'malo mwake ndi kosazama.
Kukana kutentha ndi dzimbiri bwino.
Kukana bwino kwambiri ming'alu.
Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zida zolumikizirana kwa zaka 22.
Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira aluminiyamu, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi brass, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira kaboni ndi zina zowonjezera ndi zogwiritsidwa ntchito..