E316HT1-1 Waya wozungulira wachitsulo chosapanga dzimbiri

Kufotokozera Kwachidule:

Ili ndi magwiridwe antchito abwino kwambiri monga kuwotcherera kokhazikika, kudontha pang'ono, kuchotsa matope bwino, kudyetsa waya kokhazikika, komanso mawonekedwe okongola.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

E316HT1-1 Waya wozungulira wachitsulo chosapanga dzimbiri

Mafotokozedwe Akatundu
Kugwirizana ndi muyezo: GB/T17853 E316T1-1
AWS A5.22 E316HT1-1

Makhalidwe ndi Ntchito
1. Popeza ili ndi mpweya wochuluka, ndi yoyenera kuwotcherera zida zachitsulo chosapanga dzimbiri zosagwira kutentha kwambiri;
2. Ili ndi magwiridwe antchito abwino kwambiri monga kulumikiza kokhazikika, kutayira madzi pang'ono, kuchotsa matope bwino, kudyetsa waya kokhazikika, komanso mawonekedwe okongola;
3. Chifukwa cha kuchuluka kwa Mo, kukana dzimbiri kumakhala kolimba;
4. Yoyenera kuotcherera 18%Cr-12%Ni-2%Mo m'mafakitale a petrochemical, m'ziwiya zopondereza, m'makina azachipatala ndi chakudya, feteleza ndi mafakitale ena.

Mankhwala opangidwa (wt%)

Kulemera kwa aloyi% C Mn Ndipo Cr In Mo P S Ndi
GB/T 0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.50
AWS 0.04-0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.75
Mtengo wa chitsanzo 0.50 1.45 0.50 18.05 12.00 2.35 0.020 0.005 0.05

 
Khalidwe la makina

Khalidwe la makina MPa yamphamvu yotulutsa Mphamvu yokoka ya MPa Kutalikitsa% Mtengo wokhudza J/℃
GB/T - 520 30 -
AWS - 520 30 -
Mtengo wa chitsanzo - 560 35 -

 
Mitundu yovomerezeka yamagetsi: (DC+)

Kuwotcherera waya m'mimba mwake (mm) 1.2 1.6
Voliyumu (V) 22-36 26-38
Mphamvu (A) 120-260 200-300
Kutalika kouma (mm) 15-20 18-25
Kuyenda kwa mpweya (l/min) 15-25 15-25

 
Zosamala Zowotcherera
1. Gwiritsani ntchito mpweya woteteza wa CO2 wokhala ndi chiyero cha ≥99.98% ndi mpweya woyenda wa 20-25L/min.
2. Kutentha kwa pakati pa njira: 16~100 ℃.
3. Polumikiza, ndikofunikira kuteteza ku mphepo kuti mpweya woteteza usabalalike. Mafuta, madzi, ndi zina zotero pamalo olumikizira ziyenera kuchotsedwa.
4. Gwiritsani ntchito waya wowotcherera mwamsanga mukatsegula phukusi. Ngati sunathe, chitanipo kanthu kuti zisanyowetsedwe.

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.