E70C-6M Carbon Steel Flux Cored Arc Welding Electrodes Flux Core Welding Waya

Kufotokozera Kwachidule:

Waya wowotcherera wachitsulo wa E70C-6M umaphatikiza magwiridwe antchito a mawaya olimba (GMAW) ndi kuchuluka kwa ntchito kwa mawaya okhala ndi ma flux-core (FCAW) - kuchuluka kochepa kwa utsi, mphamvu zambiri, palibe slag yoti ayeretse kapena kuchotsa - ndi zabwino zonse zomwe mawaya okhala ndi mawaya olimba ali nazo - palibe "kuzungulira kozizira" kapena kusowa kwa kugwirizanitsa kwa mbali, kupopera koyera ndi 75-80% argon/balance carbon dioxide, kuthamanga kofulumira kwa kukula kwa fillet.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Waya wowotcherera wachitsulo wa E70C-6M umaphatikiza magwiridwe antchito a mawaya olimba (GMAW) ndi kuchuluka kwa ntchito kwa mawaya okhala ndi flux-core (FCAW) - kuchuluka kochepa kwa utsi, mphamvu zambiri, palibe slag yoyeretsa kapena kuchotsa - ndi zabwino zonse zomwe mawaya okhala ndi core ali nazo kuposa mawaya olimba - palibe "kuzungulira kozizira" kapena kusowa kwa kugwirizanitsa kwa mbali, kupopera koyera ndi 75-80% argon/balance carbon dioxide, kuthamanga kofulumira kwa kukula kwa fillet. E70C-6M ndi yoyenera kugwiritsidwa ntchito komwe kuchuluka kwa manganese ndi silicon ndikofunikira, monga kukhalapo kwa chitoliro cholemera kapena zodetsa zochepa, kapena pamene kunyowetsa bwino kwa weld bead kukufunika. Chogulitsachi chimapambana kwambiri pakuwotcherera, koma chimakhala chabwino kwambiri pamikhalidwe yofunikira kwambiri monga popanga zitsulo zolemera, ntchito yomanga, kuwotcherera mapaipi ndi kuwotcherera ma heater amadzi otentha.

Kalasi ya AWS: E70C-6M Chitsimikizo: AWS A5.18/A5.18M: 2005
Aloyi: E70C-6M ASME SFA A5.18

 

Malo Owotcherera: F, H, V, OH .035-1/16”
F, H 5/64”-1/8”
Zamakono:
DCEP

 

Mphamvu Yokoka, kpsi: 70 100% CO2
Mphamvu Yopereka, kpsi: 58 100% CO2
Kutalika kwa 2”%: 22 100% CO2

Mankhwala a Waya Omwe Amagwiritsidwa Ntchito Mogwirizana ndi AWS A5.18 (Mitengo imodzi ndiyo yokwanira)

C Mn Si S P Ni Cr Mo V Cu  
0.12 1.75 0.90 0.03 0.03 0.50 0.20 0.30 0.08 0.50  
Magawo Omwe Amawotcherera Achizolowezi
M'mimba mwake Njira Volti Ma Amps Mpweya Woteteza
in (mm)
.035 (0.9) GMAW 24-35 160-250 75-95% Ar/balance Co2, 35-50cfh
.045 (1.2) GMAW 37-33 180-330 75-95% Ar/balance Co2, 35-50cfh
.052 (1.3) GMAW 25-35 220-460 75-95% Ar/balance Co2, 35-50cfh
1/16 (1.6) GMAW 26-37 240-520 75-95% Ar/balance Co2, 35-50cfh
5/64 (2) GMAW 27-36 240-550 75-95% Ar/balance Co2, 35-50cfh
3/32 (2.4) GMAW 28-36 350-550 75-95% Ar/balance Co2, 35-50cfh
7/64 (2.78) GMAW 27-34 400-600 75-95% Ar/balance Co2, 35-50cfh
1/8 (3.2) GMAW 26-32 95-145 75-95% Ar/balance Co2, 35-50cfh

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.