Waya Wowotcherera wa AWS E70T-1 CO2 Wotetezedwa ndi Gasi Wotchedwa Flux Cored

Kufotokozera Kwachidule:

Waya Wowotcherera wa AWS E70T-1 CO2 Wotetezedwa ndi Gas-Shielded Flux Cored. Umagwiritsidwa ntchito powotcherera zinthu zopangidwa ndi chitsulo cha kaboni ndi chitsulo chopangidwa ndi chitsulo chotsika chomwe chili ndi mphamvu yolimba yoposa kapena yofanana ndi 490MPa.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

AWS E70T-1 CO2 Yotetezedwa ndi GasiFlux Cored Waya wowotcherera

Amagwiritsidwa ntchito polumikiza zinthu zopangidwa ndi chitsulo cha kaboni ndi chitsulo chopangidwa ndi zinthu zochepa zokhala ndi mphamvu yokoka yoposa kapena yofanana ndi 490MPa. Amagwiritsidwa ntchito kwambiri polumikiza zinthu zina zofunika monga kupanga zombo, kupanga makina, zotengera zopanikizika, ma boiler, makina amafuta, makina a mankhwala, makina okweza, ndi zina zotero.

Kukula 0.8mm 1.0mm 1.2mm 1.6mm 2.0mm 2.4mm 3.0mm 3.2mm 4.0mm
Mapulogalamu Amagwiritsidwa ntchito polumikiza zinthu zopangidwa ndi chitsulo cha kaboni ndi chitsulo chopangidwa ndi zinthu zochepa zokhala ndi mphamvu yokoka yoposa kapena yofanana ndi 490MPa. Amagwiritsidwa ntchito kwambiri polumikiza zinthu zina zofunika monga kupanga zombo, kupanga makina, zotengera zopanikizika, ma boiler, makina amafuta, makina a mankhwala, makina okweza, ndi zina zotero.

 

Kapangidwe ka mankhwala a chitsulo chosungidwa (%)
C
≤0.18
Si
≤0.90
Mn
≤1.75
S
≤0.03
P
≤0.03

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.