E71T-GS A5.20, Carbon Steel Flux Cored Arc Welding Electrodes Flux Core Welding Wire

Kufotokozera Kwachidule:

E71T-GS ndi electrode yokhala ndi chitsulo cha kaboni, flux cored yogwiritsidwa ntchito popanda mpweya woteteza wakunja. Electrode iyi cholinga chake ndi kuwotcherera chitsulo cha kaboni chopyapyala, kuyambira 3/16” mpaka 22 gauge.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda


E71T-GS ndi electrode yokhala ndi chitsulo cha kaboni, flux cored yogwiritsidwa ntchito popanda mpweya woteteza wakunja. Electrode iyi cholinga chake ndi kuwotcherera chitsulo cha kaboni chopyapyala, kuyambira 3/16” mpaka 22 gauge.

Ntchito Zachizolowezi: zotchingira zotchingira zoyendetsedwa ndi single-pass; izi zapangidwa kuti zitchingire bwino kwambiri pa zinthu zomatira ndipo zitha kugwiritsidwanso ntchito pamalo ena opangidwa ndi aluminiyamu. E71T-GS sifunikira chitetezo chakunja cha gasi ndipo iyenera kutchingidwa ndi DCEN (straight polarity).

Kalasi ya AWS: E71T-GS Chitsimikizo: AWS A5.20/A5.20M:2005
Aloyi: E71T-GS AWS/ASME SFA A5.20

 

Kuwotcherera Udindo:
H, F, V, O
Zamakono:
DCEN
Polarity yolunjika

 

Mphamvu Yotambasula Yokoka, kpsi: Mphindi 86.4 (Kusweka kwachitsulo chapansi)
Mayeso Otsogozedwa a Bend Imakwaniritsa zofunikira za AWS

 

Magawo Awiri A Waya
M'mimba mwake Njira Ma Amps Ma Volti Liwiro la Chakudya cha Waya
in (mm)
.030″ 0.8 FCAW 50 15 80
    FCAW 100 16 225
    FCAW 150 17 375
    FCAW 175 17 445
.035″ 0.9 FCAW 75 15 70
    FCAW 100 16 110
    FCAW 150 17 180
    FCAW 200 18 305
.045″ 1.2 FCAW 100 15 70
    FCAW 150 16 120
    FCAW 200 17 195
    FCAW 225 17 245
1/6″ 1.6 FCAW 150 17 60
    FCAW 200 18 85
    FCAW 250 18 135
    FCAW 300 19 180
5/64” .078 FCAW 200 19 60
    FCAW 250 20 80
    FCAW 300 21 115
    FCAW 325 120 6.6

*Ma parameter awa angagwiritsidwe ntchito m'malo onse. Kuthekera kogwiritsa ntchito chitsulo chosungunuka pamlingo wapamwamba wamagetsi kudzadalira makulidwe a mbale ndi luso la wowotcherera.

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.