Waya Wowotcherera wa Flux Cored, Giredi: Waya Wopanda Chitsulo Wosapanga Dzimbiri wa A 5.22 E308L T1-1

Kufotokozera Kwachidule:

Pakuwotcherera zitsulo za Low Carbon 18-20% Cr/ 8-12% Ni zomwe zili ndi mphamvu yabwino kwambiri yowotcherera Chifukwa cha kukhalapo kwa ferrite, chitsulo chowotcherera chimakhala ndi mphamvu zochepa zosweka. Kapangidwe ka makina ndi kabwino kwambiri ngati kowotcherera ndipo kamakhala ndi kukana dzimbiri pakati pa tinthu tating'onoting'ono chifukwa cha kuchuluka kwa kaboni kochepa.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Flux Cored Waya wowotchereraGiredi: A 5.22 E308l T1-1

Mafotokozedwe a Zamalonda

Zida Zazida SS
Kuchuluka Pa Mpukutu uliwonse makilogalamu 15
Kulongedza 15 kg pa paketi iliyonse
Giredi A 5.22 E308L T1-1
Mtundu wa Phukusi Chikwama chotsekedwa mu thumba la polyethylene ndipo chodulidwacho chikukulungidwa mu bokosi lozungulira
Kukhuthala 1.2MM 1.6MM
Zamakono 190-300A
Kukulitsa Waya 20-25mm (yopindika)
Kukula Kopezeka 2.00mm, 2.4mm
Polarity Waya wabwino wa DC
Mpweya Woteteza Mpweya wa CO2 wokhala ndi liwiro la malita 15-20 pa mphindi
Katundu wa Makina Osenda UTS=520N/mm2 Mphindi; Kutalika(%)=35% mphindi
Kusungunula chitsulo cha chemistry C= 0.035%,Mn=1.65%,P=0.02%,Si=0.50%,S=0.008%,Ni=9.50%,Cr=19.50%

Mafotokozedwe Akatundu
Waya wosapanga dzimbiri wopangidwa ndi chitsulo chosapanga dzimbiri wokhala ndi arc yokhazikika komanso yosalala, yokhala ndi slag detachability yabwino

Mapulogalamu:
Pakuwotcherera zitsulo za Low Carbon 18-20% Cr/ 8-12% Ni zomwe zili ndi mphamvu yabwino kwambiri yowotcherera Chifukwa cha kukhalapo kwa ferrite, chitsulo chowotcherera chimakhala ndi mphamvu zochepa zosweka. Kapangidwe ka makina ndi kabwino kwambiri ngati kowotcherera ndipo kamakhala ndi kukana dzimbiri pakati pa tinthu tating'onoting'ono chifukwa cha kuchuluka kwa kaboni kochepa.

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.