Ma Electrode Abwino Kwambiri Owelda a Tyue Brand AWS A5.4 E320-16 a Chitsulo Chosapanga Dzira

Kufotokozera Kwachidule:

A902 (AWS E320-16) ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi zokutira za titaniyamu-calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi

A902

GB/T E320-16

AWS A5.4 E320-16

Kufotokozera: A902 ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi zokutira za titaniyamu-calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri. Chitsulo chake chosungidwa chili ndi kukana dzimbiri komanso kukana kwamphamvu kwa okosijeni ndipo chimagwiritsidwa ntchito kwambiri popanga zida zamafakitale, mafuta, ndi hydrogen.

Kugwiritsa Ntchito: Kugwiritsidwa ntchito powotcherera Carpenter20Cb nickel alloy mu sulfuric acid, nitric acid, phosphoric acid ndi oxidative acid corrosion medium. Kungagwiritsidwenso ntchito powotcherera zitsulo zosiyanasiyana.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Si

Mn

Cr

Ni

Mo

Cu

Nb

S

P

≤0.07

≤0.60

0.5 ~ 2.5

19.0 ~ 21.0

32.0 ~ 36.0

2.0 ~ 3.0

3.0 ~ 4.0

8 XC ~ 1.00

≤0.030

≤0.030

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

 Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥550

≥30

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

()mm)

2.5

3.2

4.0

kuwotcherera Current

()A)

50 ~ 80

80 ~ 110

110 ~ 160

 

Zindikirani:

  1. Elektrodi iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 150℃ isanayambe kuwotcherera;
  2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yogwiritsa ntchito AC welding, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse.

 

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 