Ma Electrode Omwe Amawotcherera AWS A5.4 E310Mo-16 Zitsulo Zosapanga Zitsulo Zowotcherera Ndodo Zomatira Ma Electrode

Kufotokozera Kwachidule:

A412 (AWS E310Mo-16) ndi electrode yachitsulo chosapanga dzimbiri ya Cr26Ni21Mo2 yokhala ndi titaniyamu calcium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi

A412                                 

GB/T E310Mo-16

AWS A5.4 E310Mo-16

Kufotokozera: A412 ndi electrode yachitsulo chosapanga dzimbiri ya Cr26Ni21Mo2 yokhala ndi titaniyamu ya calcium. Ingagwiritsidwe ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri. Chifukwa chakuti molybdenum imawonjezedwa ku chitsulo chosungidwa, kukana kwake kuyika dzenje, mphamvu ya kutentha, komanso kukana ming'alu zonse zimawonjezeka poyerekeza ndi A402 ndi A407.

Kugwiritsa Ntchito: Imagwiritsidwa ntchito polumikiza chitsulo chosapanga dzimbiri chosagwira kutentha chomwe chimagwira ntchito pa kutentha kwambiri, ndipo ingagwiritsidwenso ntchito polumikiza zingwe zachitsulo chosapanga dzimbiri, zitsulo zosiyana, ndi zina zotero. Imakhala ndi kukana bwino ming'alu ikalumikiza chitsulo cha kaboni ndi chitsulo chotsika cha alloy chomwe chimalimba kwambiri.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.030

 

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥550

≥25

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.0

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Zindikirani:

  1. Elektrodi iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 150℃ isanayambe kuwotcherera;
  2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yogwiritsa ntchito AC welding, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse.

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 

 

 