Chitsulo chosapanga dzimbiri chowotcherera maelekitirodi
A022
GB/T E316L-16
AWS E316L-16
Kufotokozera: A022 ndi electrode yachitsulo chosapanga dzimbiri ya Cr18Ni12Mo2 yokhala ndi kaboni wochepa kwambiri yokhala ndi titaniyamu ya calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino. Kaboni yomwe ili mu chitsulo chosungidwa ndi ≤0.04%, zomwe zimapangitsa kuti ikhale yolimba kutentha, yolimba dzimbiri komanso yolimba ming'alu.
Kugwiritsa Ntchito: Amagwiritsidwa ntchito polumikiza urea, ulusi wopangidwa ndi zipangizo zina komanso mtundu womwewo wa kapangidwe ka chitsulo chosapanga dzimbiri. Angagwiritsidwenso ntchito pa chitsulo chosapanga dzimbiri cha chromium, chitsulo chophatikizika ndi chitsulo chosiyana chomwe sichingathe kutenthedwa pambuyo polumikiza.
Kapangidwe ka mankhwala a chitsulo chosungunula (%):
| C | Mn | Si | Cr | Ni | Mo | Cu | S | P |
| ≤0.04 | 0.5 ~ 2.5 | ≤0.90 | 17.0 ~ 20.0 | 11.0 ~ 14.0 | 2.0 ~ 3.0 | ≤0.75 | ≤0.030 | ≤0.040 |
Kapangidwe ka makina a chitsulo chosungunula:
| Chinthu choyesera | Kulimba kwamakokedwe Mpa | Kutalikitsa % |
| Chotsimikizika | ≥490 | ≥30 |
Mphamvu yovomerezeka:
| M'mimba mwake wa ndodo (mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 |
| kuwotcherera Current (A) | 25 ~ 50 | 50 ~ 80 | 80 ~ 110 | 110 ~ 160 | 160 ~ 200 |
Zindikirani:
1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 150℃ isanayambe kuwotcherera;
2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yolumikiza magetsi a AC, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse;
3. Kukana dzimbiri kwa chitsulo chosungidwa kumatsimikiziridwa ndi mgwirizano wawiri wa kupereka ndi kufuna.
Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.
Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.