Waya Wowotcherera wa AWS A5.7 ERCuSn-C wa Copper Alloy Waya Wowotcherera wa Mkuwa

Kufotokozera Kwachidule:

Waya wa mkuwa wa AWS A5.7 ERCuSn-C Phosphor ndi wopangidwa ndi bronze womwe umagwiritsidwa ntchito polumikiza mkuwa ndi aloyi ya Cu-Sn.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Waya wa mkuwa wa AWS A5.7 ERCuSn-C Phosphor

Chiyambi
Akulimbikitsidwa kugwiritsa ntchito kulumikiza mkuwa ndi Cu-Sn alloy. Abwino kwambiri kugwiritsa ntchito kulumikiza mkuwa ndi chitsulo. Akulimbikitsidwa kugwiritsa ntchito kutentha pasadakhale pazinthu zazikulu, ndipo kulumikiza kwa argon arc ndi pulsed kumalimbikitsidwa kugwiritsa ntchito kulumikiza kwa multilayer hard facing pa chitsulo.

Kukhazikitsa miyezo:   Chizindikiro cha Manambala:
GB/T9460-2008   SCu5210
AWS A5.7:2007   ERCuSn-C
BS EN14640:2005   Cu 5210
     
Kapangidwe (miyezo yokhazikika):   %
Cu incl.ag   bal.
Zn   0.20
Sn   7.00-9.00
Fe   0.10
P   0.10-0.35
Al   0.01
Pb   0.02
Ena onse   0.50
     
Kapangidwe ka zinthu zakuthupi:    
Kuchulukana Kg/m3 8.8
Malo osungunuka ℃ 875-1025
Kutentha kwa matenthedwe W/mK 66
Kuyendetsa magetsi Sm/mm2 6-8
Kuchuluka kwa kutentha koyenera 10^-6/K(20-300℃) 18.5
     
Miyezo yokhazikika ya chitsulo chosungunula:    
Kutalikitsa % 20
Kulimba kwamakokedwe N/mm2 260
Ntchito yokhudza kukhudza mipiringidzo ya notched bar J 32
Kuuma kwa Brinell HB 2.5/62.5 80
     
Mapulogalamu:    
Chotsukira cha mkuwa cha aluminiyamu wokhuthala kwambiri wa aluminiyamu wopangira chowumitsira pamwamba. Choyenera makamaka kuwotcherera zinthu zamkuwa, monga mkuwa, bronze wa aluminiyamu, makamaka chogwiritsidwa ntchito polumikiza zitsulo zamkuwa ndi zitsulo. Choyenera kuwotcherera ma bronze opangidwa ndi chitsulo komanso chosungunula mu uvuni. Pa kuwotcherera kwa multilayer pa chitsulo, kuwotcherera kwa arc wopukutidwa kumalimbikitsidwa. Pa zinthu zazikulu zogwirira ntchito, kutentha koyambirira kumalimbikitsidwa.
     
Makongoletsedwe:    
M'mimba mwake: 0.64 – 0.80 – 1.00 – 1.20 – 1.60 –2.40
Ma Spools: D100, D200, D300, D760, K300, KS300
Ndodo: 1.60 – 9.6 mm x 914/1000 mm
Ma electrode alipo.
Zodzoladzola zina zikapemphedwa.

Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 

 

 

 