AWS E309L-15 Ndodo Zowotcherera Zosapanga dzimbiri, Zopangira zitsulo zosapanga dzimbiri Arc Welding Electrode

Kufotokozera Kwachidule:

A067 (AWS E309L-15) ndi low-hydrogen sodium mtundu Ultra-low carbon Cr23Ni13 stainless steel electrode.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Welding Stainless Steel WeldingElectrode

A067                                         

GB/T E309L-15

AWS E309L-15

Kufotokozera: A067 ndi otsika-hydrogen sodium mtundu Ultra-low carbon Cr23Ni13 zosapanga dzimbiri electrode.Gwiritsani ntchito DCEP (mwachindunji pakalipano ma elekitirodi abwino) ndipo mutha kuwotcherera m'malo onse.Lili ndi mpweya wochepa kwambiri, kotero umatha kukana dzimbiri la intergranular chifukwa cha mpweya wa carbide popanda stabilizers monga niobium ndi titaniyamu.

Ntchito: Amagwiritsidwa ntchito pamtundu womwewo wa zitsulo zosapanga dzimbiri, zitsulo zophatikizika ndi zitsulo zooneka ngati zapadera popanga ulusi wopangira, petrochemical ndi zida zina.Itha kugwiritsidwanso ntchito poyang'ana zigawo zosinthira pakhoma lamkati la zombo zamphamvu zanyukiliya ndi kuwotcherera zida zamkati za nsanja.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Elongation

%

Zotsimikizika

≥520

≥25

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50-70

80-120

130 ~ 160

160 ~ 200

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 300 ℃ isanayambe ntchito yowotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, sikelo yamafuta, madzi, ndi zonyansa pazigawo zowotcherera musanayambe kuwotcherera.

 

Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelectrode kuwotchereras, ndodo zowotcherera,ndikuwotcherera consumableskwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo zitsulo zosapanga dzimbirielectrode kuwotchereras, mpweya zitsulo kuwotcherera maelekitirodi, low aloyi kuwotcherera maelekitirodi, surfacing ma elekitirodi kuwotcherera, faifi tambala & cobalt aloyi kuwotcherera maelekitirodi, wofatsa zitsulo & otsika aloyi mawaya kuwotcherera, zitsulo zosapanga dzimbiri kuwotcherera mawaya, mpweya wotetezedwa flux cored mawaya, aluminium kuwotcherera mawaya, kumizidwa arc kuwotcherera .mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.