Ma Electrode Owelda a AWS E309Mo-16 a Chitsulo Chosapanga Dzimbiri, Ndodo Zabwino Kwambiri Zowelda za Arc

Kufotokozera Kwachidule:

A312 (AWS E309Mo-16) ndi electrode yachitsulo chosapanga dzimbiri ya Cr23Ni13Mo2 yokhala ndi titaniyamu calcium yokutira.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi

A312                                     

GB/T E309Mo-16

AWS A5.4 E309Mo-16

Kufotokozera: A312 ndi electrode yachitsulo chosapanga dzimbiri ya Cr23Ni13Mo2 yokhala ndi titaniyamu ya calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri. Ili ndi kukana dzimbiri, ming'alu, komanso okosijeni kuposa A302 chifukwa chitsulo chosungidwacho chili ndi molybdenum.

Kugwiritsa Ntchito: Imagwiritsidwa ntchito polumikiza chidebe chachitsulo chosapanga dzimbiri chomwe chimalimbana ndi dzimbiri ndi sulfuric acid medium (ammonia sulfide), ndipo ingagwiritsidwenso ntchito polumikiza chidebe chachitsulo chosapanga dzimbiri, mbale yachitsulo yophimbidwa ndi chitsulo chosiyana.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥550

≥25

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.0

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Zindikirani:

  1. Elektrodi iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 150℃ isanayambe kuwotcherera;
  2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yogwiritsa ntchito AC welding, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse.

 

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode owotcherera,ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 


  • Yapitayi:
  • Ena: