E9015-B3 chitsulo chowotcherera chotsika cha alloy

Kufotokozera Kwachidule:

Ma Electrode a Zitsulo Zosagonja


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

AWS: SFA 5.5 E9015-B3Ma Electrode a Zitsulo Zosagonja

Ma electrode otsika a haidrojeni 2.25Cr - 1Mo amatulutsa chitsulo, amawonetsa mphamvu zodabwitsa komanso kukana kugwedezeka pa kutentha kokwera mpaka 575 C. Amagwiritsidwa ntchito polumikiza chitsulo cholimba cha 21⁄4 Cr-1 Mo ndi zitsulo za Cr-Mo-V zomwe sizimakhudzidwa ndi haidrojeni pansi pa kukakamizidwa komanso zitsulo zopangidwa ndi chitsulo chofanana ndi zitsulo zosungunuka. Ntchito zambiri zimaphatikizapo kupanga boiler ya nthunzi, kuwotcherera mapaipi a nthunzi ndi superheater, malo opangira magetsi, malo oyeretsera mafuta ndi malo opangira mankhwala.

KUPANGIDWA KWA MANKHWALA A CHITSULO CHONSE CHOWEDWA (%)

Chinthu C Mn Si P S Cr Mo
Peresenti 0.05-0.12 0.5-0.9 ≤0.5 ≤0.030 0.022 2.0-2.5 0.9-1.2

KATUNDU WA MAKANIKO A CHITSULO CHONSE CHOWEDWA

(PWHT: 690°C KWA 1 HR)

UTS YS Kutalikitsa
(MPa) (MPa) (L = 4d)%
≥590 550 ≥15

DATA YATSOPANO NDI YOPAKITSA: DC (+)

Kukula (mm)

5×450

4×450

3.15×450

2.5×350

Mitundu Yamakono (Amps)

200-250

150-190

100-140

70-100

Kuchuluka (Zidutswa/Katoni)

35

55

75

100

Chenjezo

1. Kuumitsanso ma electrode pa 250-300 C kwa ola limodzi, malinga ndi momwe timachitira nthawi zonse.

2. Gwiritsani ntchito mkanda waufupi komanso wozungulira.