Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi
A032Mo
GB/T E317L-16
AWS E317L-16
Kufotokozera: A032Mo ndi electrode yachitsulo chosapanga dzimbiri ya Cr19Ni13Mo3 yokhala ndi kaboni yochepa kwambiri yokhala ndi titaniyamu ya calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino. Kukana dzimbiri ku sulfuric acid, sulfurous acid ndi organic acid kuli bwino kuposa kwa E316L.
Kugwiritsa Ntchito: Imagwiritsidwa ntchito polumikiza zinthu zachitsulo chosapanga dzimbiri monga AISI317 ndi 317L, ndipo ndi yoyeneranso kulumikiza ndi kuyika pamwamba pa zitsulo zopangidwa ndi chitsulo chosakanikirana ndi chitsulo chooneka ngati chapadera zomwe sizingagwedezeke ndi dzimbiri.
Kapangidwe ka mankhwala a chitsulo chosungunula (%):
| C | Mn | Si | Cr | Ni | Mo | Cu | S | P |
| ≤0.04 | 0.5 ~ 2.5 | ≤0.90 | 18.0 ~ 21.0 | 12.0 ~ 14.0 | 3.0 ~ 4.0 | ≤0.75 | ≤0.030 | ≤0.040 |
Kapangidwe ka makina a chitsulo chosungunula:
| Chinthu choyesera | Kulimba kwamakokedwe Mpa | Kutalikitsa % |
| Chotsimikizika | ≥520 | ≥25 |
Mphamvu yovomerezeka:
| M'mimba mwake wa ndodo (mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 |
| kuwotcherera Current (A) | 25 ~ 50 | 50 ~ 80 | 80 ~ 110 | 110 ~ 160 | 160 ~ 220 |
Zindikirani:
1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha pafupifupi 250℃ isanayambe kuwotcherera;
2. Ndikofunikira kuyeretsa dzimbiri, mafuta oyeretsera, madzi, ndi zinyalala pa zipangizo zowotcherera musanawotchetse.
Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.
Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.