AWS E430-16 Stainless Steel Welding ElectrodeManual Metal Arc Electrodes, Best Welding Consumables Supplier

Kufotokozera Kwachidule:

G302 (AWS E430-16) ndi Cr17 chitsulo chosapanga dzimbiri electrode yokhala ndi zokutira titaniyamu-calcium.Itha kugwiritsidwa ntchito ndi AC ndi DC.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Welding Stainless Steel WeldingElectrode

G302                                                  

GB/T E430-16

AWS E430-16 

Kufotokozera: G302 ndi Cr17 zitsulo zosapanga dzimbiri electrode yokhala ndi titaniyamu-calcium zokutira.Itha kugwiritsidwa ntchito ndi AC ndi DC.

Ntchito: Ntchito kuwotcherera dzimbiri zosagwira (nitric acid) ndi zosagwira kutentha Cr17 zitsulo zosapanga dzimbiri nyumba.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.10

≤1.0

≤0.90

15.0 ~ 18.0

≤0.6

≤0.75

≤0.75

≤0.03

≤0.04

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Elongation

%

Zotsimikizika

≥450

≥20

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

3.2

4.0

5.0

Welding Current

(A)

80-120

100 ~ 160

150 ~ 200

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 150 ℃ isanayambe ntchito yowotcherera;

2. Gawo la welded liyenera kutenthedwa pa 200 ° C musanayambe kuwotcherera.

 

Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelectrode kuwotchereras, ndodo zowotcherera,ndikuwotcherera consumableskwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 