AWS E7015-G Low Temperature Steel Welding Electrode W607 Low-Hydrogen Welding Rod

Kufotokozera Kwachidule:

W607 (AWS E7015-G) ndi electrode yachitsulo yotsika kutentha yokhala ndi zokutira za hydrogen sodium.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Low Kutentha Zitsulo kuwotcherera Electrode

W607                                                     

GB/T E5015-G

AWS A5.5 E7015-G

 

Kufotokozera: W607 ndi electrode yachitsulo yotsika kutentha yokhala ndi zokutira za hydrogen sodium.Gwiritsani ntchito DCEP (mwachindunji pakalipano ma elekitirodi abwino) ndipo mutha kuwotcherera m'malo onse.Chitsulo choyikidwa chimakhala ndi mphamvu yabwino pa -60 ° C.

Ntchito: Ntchito kuwotcherera otsika kutentha zitsulo monga 09MnD.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Mtengo (J)

-60 ℃

Zotsimikizika

≥490

≥390

≥22

≥27

 

Kuphatikizika kwa haidrojeni muzitsulo zoyikidwa: ≤6.0mL/100g (njira ya glycerin) kapena ≤10mL/100g (njira ya mercury kapena gas chromatography)

Kuwunika kwa X-ray: Ndimapanga

 

Zomwe tikulimbikitsidwa:

(mm)

Ndodo diameter

2.0

2.5

3.2

4.0

5.0

(A)

Welding Current

40-70

60-90

100 ~ 120

140 ~ 170

170 ~ 200

 

Zindikirani:

1. Elekitirodi ayenera kuphika kwa ola 1 pa 350 ℃ pamaso kuwotcherera ntchito;

2. Ndikofunikira kuyeretsa dzimbiri, sikelo yamafuta, madzi, ndi zonyansa pazigawo zowotcherera musanawotchere;

3. Gawo la welded likhoza kutenthedwa pa 150 ° C musanawotchere kuti zisawonongeke.

 