AWS E7015 ndodo zowotcherera

Kufotokozera Kwachidule:

AWS A5.1 E7015 ndi low-hydrogen sodium yokutidwa carbon steel electrode.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

AWS A5.1 E7015 ndi low-hydrogen sodium yokutidwa carbon steel electrode.

Elekitirodi yowotcherera ya E7015 iyenera kugwiritsidwa ntchito pa DCEP.Ili ndi ma welding abwino kwambiri omwe amawathandiza kuti azitha kuwotcherera malo onse, ali ndi arc yokhazikika, kuchotsa slag ndikosavuta komanso kumakhala ndi spatter yochepa.Chitsulo choyikidwa chimakhala ndi machitidwe abwino amakina komanso kukana ming'alu, zomwe zimapereka kulimba kwa kutentha kochepa.

Kugwiritsa ntchito

AWS A5.1 E7015 imagwiritsidwa ntchito powotcherera zitsulo zapakati-carbon ndi zocheperako monga 16Mn, 09Mn2Si, 09Mn2V ndi zitsulo zomwe zimagwiritsidwa ntchito popanga zombo monga A, B, D, E. Amagwiritsidwanso ntchito m'mbale zachitsulo zokhuthala ndi zida za carbon steel zomwe zimakhala zovuta kuwotcherera.

Gwirizanani ndi Standard

GB/T 5117 E5015

AWS A5.1 E7015

ISO 2560-BE 49 15 A

Cholinga:AWS A5.1 E7015 imagwiritsidwa ntchito powotcherera zitsulo zapakati pa kaboni ndi zinthu zochepa za alloy monga 16Mn, 09Mn2Si, 09Mn2V ndi zitsulo zomwe zimagwiritsidwa ntchito popanga zombo monga A, B, D, E. Amagwiritsidwanso ntchito muzitsulo zokhuthala mbale ndi zida za carbon steel zomwe zimakhala zovuta kuwotcherera.

Mapangidwe a Chemical (%)

Chemical Composition

C

Mn

Si

S

P

Ni

Cr

Mo

V

Mtengo wa Guarantee

≤

0.15

≤

1.60

≤

0.90

≤0.035

≤0.035

≤

0.30

≤

0.20

≤

0.30

≤

0.08

Zotsatira Zonse

0.082

1.10

0.58

0.012

0.021

0.011

0.028

0.007

0.016

Mechanical Properties of Deposited Metal(Gasi Woteteza:CO2)

Chinthu Choyesera

Rm (MPa)

ReL (MPa)

A(%)

KV2(J)

-20 ℃ -30 ℃

Mtengo wa Guarantee

≥490

≥400

≥20

≥47

≥27

Zotsatira Zonse

550

450

32

150

142

Zofunikira Zoyeserera za X-Ray: Gulu I

Reference Current (DC+)

Diameter(mm)

Φ2.5

Φ3.2

Φ4.0

Φ5.0

Amperage (A)

60-100

80-140

110-210

160-230

Ndemanga:

1. Elekitirodi iyenera kutenthedwa pa kutentha kwa 350 ° C kwa ola limodzi.Preheat ndodo nthawi iliyonse ikagwiritsidwa ntchito.

2. Zonyansa monga dzimbiri, madontho amafuta ndi chinyezi ziyenera kuchotsedwa pa ntchitoyo.

3. Short arc chofunika kuchita kuwotcherera.Njira yopapatiza yowotcherera ndiyokonda.


  • Zam'mbuyo:
  • Ena: