AWS E6011 kuwotcherera elekitirodi ndi mtundu wa mapadi potaziyamu, amene ntchito ofukula pansi kuwotcherera.Zonse za AC ndi DC kuwotcherera.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

AWS E6011electrode kuwotchererandi mtundu wa potaziyamu wa cellulose, womwe umagwiritsidwa ntchito powotcherera moyima pansi.Zonse za AC ndi DC kuwotcherera.Iwo utenga patsogolo luso yachilendo ndipo ali kwambiri kuwotcherera katundu luso.Utali wa ARC uyenera kuyendetsedwa munjira yoyenera.Sikuti kuwotcherera multilayer ndi chivundikiro kuwotcherera.

Kugwiritsa ntchito

Ndodo zowotcherera AWS E6011 ndizoyenera kuwotcherera zotengera zotengera monga nyumba ndi milatho, akasinja osungira, mapaipi ndi zotengera zokakamiza.

MAWONEKEDWE:

Mwamsanga-kuyambira bwino

Superior arc drive

Slag imatuluka mosavuta

Zabwino kwambiri zonyowetsa ZABWINO:

Kugunda kosavuta kwa arc, koyenera kunyamula

Kulowa kwabwino

Kuyeretsa mwachangu

Kuwoneka bwino kwa mikanda, kumachepetsa kuzizira komanso kudulidwa

MTUNDU WA TSOPANO: Direct Current Electrode Positive (DCEP) kapena AC

NJIRA ZOYENERA ZOWESETSA:

Arc Length - Avereji yautali (1/8" mpaka 1/4")

Lathyathyathya - Khalani patsogolo pa chithaphwi ndikugwiritsa ntchito kukwapula pang'ono

Chopingasa - Elekitirodi yolowera pang'ono kumtunda

Vertical Up - Kukwapula pang'ono kapena kuluka

Vertical Down - Gwiritsani ntchito mayendedwe okwera komanso kuyenda mwachangu, kukhala patsogolo pamadzi

Pamwamba - Khalani patsogolo pa chithaphwi ndikugwiritsa ntchito kukwapula pang'ono

Kupanga Kwamankhwala (%)

C Mn Si S P
<0.12 0.3-0.6 <0.2 <0.035 <0.04

Mechanical Properties of Deposited Metal

Chinthu Choyesera

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Mtengo wa Guarantee

≥460

≥330

≥16

≥47

Zotsatira Zonse

485

380

28.5

86

Reference Current (DC)

Diameter

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40-70

50-90

90-130

130 ~ 210

170 ~ 230

Chenjerani:

1. Ndikosavuta kuwonetsa chinyezi, chonde sungani pamalo owuma.

2. Imafunika kutenthetsa pamene phukusi likusweka kapena chinyezi chimalowa, kutentha kwa kutentha kuyenera kukhala pakati pa 70C mpaka 80C, nthawi yotentha iyenera kukhala kuyambira 0.5 mpaka 1 ora.

3. Mukamagwiritsa ntchito ma elekitirodi owotcherera a 5.0mm, ndikwabwino kugwiritsa ntchito zida zapamwamba, zotsika, kuti muwonjezere magwiridwe antchito.