Ni307-4 (AWS ENiCrFe-4) ndi electrode yochokera ku nickel yokhala ndi zokutira za hydrogen sodium.Gwiritsani ntchito DCEP (mwachindunji panopa electrode positive).


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Nickel ndiNickel Alloy Welding Electrode

N307-4                                                     

GB/T ENi6093

AWS A5.11 ENCrFe-4

 

Kufotokozera: Ni307-4 ndi electrode yochokera ku nickel yokhala ndi zokutira za hydrogen sodium.Gwiritsani ntchito DCEP (elekitirodi yamakonozabwino).Ili ndi ntchito yabwino kwambiri yowotcherera yokhala ndi kuyaka kokhazikika kwa arc, sipatter yochepa, kuchotsa mosavuta slag,

ndi weld wokongola.

 

Ntchito: Iwo ntchito kuwotcherera nickel-chromium-chitsulo aloyi, monga Ni600, Ni800/800H ndi ofanana kapena faifi tambala ofotokoza superalloys ndi kutentha ntchito 900 ° C. Angagwiritsidwenso ntchito kwa otsika-kutentha zitsulo munali Ni3% ~ 9%, monga ASTM A333, A334, A353, A522, The kuwotcherera A553 Angagwiritsidwenso ntchito dissimilar zitsulo kuwotcherera pakati Mo400, Ni825, zitsulo zosapanga dzimbiri ndi otsika aloyi chitsulo.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Fe

Si

Ni

Cr

Mo

Nb + Ta

S

P

≤0.20

1.0 ~ 5.0

≤12.0

≤1.0

≥60.0

13.0 ~ 17.0

1.0 ~ 3.5

1.0 ~ 3.5

≤0.015

≤0.020

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Zotsimikizika

≥650

≥360

≥18

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

2.5

3.2

4.0

Welding panopa

(A)

60-90

80-110

110 ~ 150

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 300 ℃ isanayambe ntchito yowotcherera;

2. M'pofunika kuyeretsa dzimbiri, mafuta, madzi, ndi zonyansa pazigawo zowotcherera musanayambe kuwotcherera.Yesani kugwiritsa ntchito arc yayifupi kuti muwotchere.

 

 


  • Zam'mbuyo: