Ndodo zowotcherera AWS A5.1 E6013 (J421)

Kufotokozera Kwachidule:

Kuwotcherera ndodo AWS A5.1 E6013 (J421) ndi oyenera kuwotcherera dongosolo otsika mpweya zitsulo, makamaka kuwotcherera wa woonda mbale zitsulo ndi yochepa discountinuous kuwotcherera ndi lamulo lachiphaso yosalala kuwotcherera.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Kuwotcherera ndodo AWS A5.1 E6013 (J421) ndi oyenera kuwotcherera dongosolo otsika mpweya zitsulo, makamaka kuwotcherera wa woonda mbale zitsulo ndi yochepa discountinuous kuwotcherera ndi lamulo lachiphaso yosalala kuwotcherera.

Magulu:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Makhalidwe:

AWS A5.1 E6013 (J421) ndi rutile mtundu electrode.Kutha kuwotcherera onse AC & DC magetsi gwero ndipo akhoza kukhala malo onse.Iwo ali kwambiri kuwotcherera ntchito monga khola arc, sipatter pang'ono, zosavuta slag kuchotsa ndi reignition-luso etc. Rutile-cellulosic elekitirodi ndi luso weld wabwino m'malo onse kuphatikizapo ofukula pansi.Kuthekera kwabwino kwambiri kwapang'onopang'ono komanso luso lodabwitsa la arc.Kwa kuwotcherera tack ndi katundu fit ups.Cholinga chachikulu chamakampani ndi malonda, kusonkhanitsa ndi kuwotcherera masitolo.

Chenjerani:

Nthawi zambiri, simuyenera kuwumitsanso ma elekitirodi musanayambe kuwotcherera.Ikakhudzidwa ndi chinyezi, iyenera kuwumitsanso pa 150 ℃-170 ℃ kwa ola la 0.5-1.

Malo Welding:

PA, PB, PC, PD, PE, PF

AWS A5.1 E6013 ndi yoyenera kuwotcherera nyumba zopangidwa ndi chitsulo chochepa cha carbon, imachita bwino kwambiri pakuwotcherera mbale zoonda komanso zazing'ono zazing'ono zachitsulo komanso imakhala ndi ntchito yabwino kwambiri yomwe imafunikira mawonekedwe abwino komanso oyera.

Mapangidwe a Chemical a All Weld Metal: (%)

Chemical Composition

C

Mn

Si

S

P

Ni

Cr

Mo

V

Zofunikira

≤0.10

0.32-0.55

≤0.30

≤0.030

≤0.035

≤0.30

≤0.20

≤0.30

≤0.08

Zotsatira Zofananira

0.08

0.37

0.18

0.020

0.025

0.030

0.035

0.005

0.004

Mechanical Properties of Deposited Metal

Chinthu Choyesera

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Zofunikira

440-560

≥355

≥22

≥47

Zotsatira Zofananira

500

430

27

80

Reference Current (DC)

Diameter

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40-70

50-90

80-130

150 ~ 210

180 ~ 240

X-Ray Radiographic Inspection:

mlingo Ⅱ


  • Zam'mbuyo:
  • Ena: