Low Alloy Steel Welding Electrode AWS E9016-D1

Kufotokozera Kwachidule:

J606 (AWS E9016-D1) ndi electrode yachitsulo yotsika kwambiri yokhala ndi chitsulo chochepa cha hydrogen potaziyamu.Itha kugwiritsidwa ntchito pakuwotcherera malo onse ndi AC ndi DC.Kukhazikika kwa kuwotcherera kwa AC ndikocheperako poyerekeza ndi kuwotcherera kwa DC.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Low Alloy Steel Welding Electrode

J606                                       

GB/T E6016-D1

AWS E9016-D1 

 

Kufotokozera: J606 ndi otsika aloyi mkulu-mphamvu zitsulo electrode ndi otsika-hydrogen potaziyamu zokutira.Itha kugwiritsidwa ntchito pakuwotcherera malo onse ndi AC ndi DC.Kukhazikika kwa kuwotcherera kwa AC ndikocheperako poyerekeza ndi kuwotcherera kwa DC. 

Ntchito: Ntchito kuwotcherera sing'anga mpweya zitsulo ndi otsika aloyi mkulu-mphamvu zitsulo nyumba lolingana mphamvu, monga Q420, etc.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Mtengo (J)

-30 ℃

Zotsimikizika

≥590

≥490

≥15

≥27

Kuyesedwa

620-680

≥500

20-28

≥27

 

Kuphatikizika kwa haidrojeni muzitsulo zoyikidwa: ≤4.0mL/100g (njira ya glycerin)

Kuwunika kwa X-ray: Ndimapanga

 

Zomwe tikulimbikitsidwa:

(mm)

Ndodo diameter

2.0

2.5

3.2

4.0

5.0

5.8

(A)

Welding Current

40-70

70-90

90-120

140 ~ 180

180 ~ 220

210 ~ 260

 

Zindikirani:

1. Elekitirodi ayenera kuphika kwa ola 1 pa 350 ℃ pamaso kuwotcherera ntchito;

2. Ndikofunikira kuyeretsa dzimbiri, sikelo yamafuta, madzi, ndi zonyansa pazigawo zowotcherera musanawotchere;

3. Gwiritsani ntchito kachipangizo kakang'ono powotcherera.Njira yopapatiza yowotcherera ndiyoyenera;

4. Mbali yowotcherera ikakhala yokhuthala, iyenera kutenthedwa mpaka 150 ° C ndikuzizidwa pang'onopang'ono mutatha kuwotcherera.

 