AWS E8016-B2 Kuweta Chitsulo Chosatentha Electrode R306 Ndodo Zoweta Zitsulo Zotsika za Hydrogen

Kufotokozera Kwachidule:

R306 (AWS E8016-B2) ndi electrode yachitsulo yolimba yolimbana ndi kutentha yokhala ndi potaziyamu yochepa ya haidrojeni yokhala ndi 1% Cr - 0.5% Mo.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Chitsulo Chosatentha cha Molybdenum ndi Chromium MolybdenumkuwotchereraElekitirodi

R306                                                     

GB/T E5516-B2

AWS A5.5 E8016-B2

Kufotokozera: R306 ndi electrode yachitsulo yolimba yolimbana ndi kutentha yokhala ndi potaziyamu yochepa ya haidrojeni yokhala ndi 1% Cr - 0.5% Mo. AC ndi DC zonse zingagwiritsidwe ntchito, ndipo zitha kuwotcherera m'malo onse. Chowotchereracho chiyenera kutenthedwa mpaka 160 ~ 250°C chisanawotchetsedwe.

Kugwiritsa Ntchito: Kugwiritsidwa ntchito powotcherera Cr 1% – Mo 0.5% chitsulo chosagwira kutentha chomwe kutentha kwake kuli pansi pa 520℃, monga mapaipi a boiler, ziwiya zopondereza, zotenthetsera ndi zida zoyeretsera mafuta, ndi zina zotero.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.60

0.80 ~ 1.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Mphamvu yobereka

Mpa

Kutalikitsa

%

Mtengo wa zotsatira (J)

Kutentha Kwabwinobwino.

Chotsimikizika

≥540

≥440

≥17

≥47

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

60 ~ 90

90 ~ 130

140 ~ 180

180 ~ 210

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 350℃ isanayambe kuwotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, mafuta oyeretsera, madzi, ndi zinyalala pa zipangizo zowotcherera musanawotchetse.

 

 


  • Yapitayi:
  • Ena: