AWS E8018-B2 Chromium Molybdenum Kuwotcherera Kutentha Kwachitsulo Electrode R306Fe Ndodo Electrodes Welding Consumables

Kufotokozera Kwachidule:

R306Fe (AWS E8018-B2) ndi pearlitic chitsulo chosagwira kutentha electrode ndi ufa wachitsulo ndi zokutira zamtundu wa hydrogen potassium zomwe zili ndi 1% Cr - 0.5% Mo.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Molybdenum ndi Chromium Molybdenum Heat Resistant Steel Welding Electrode

R306 pa                                                     

GB/T E5518-B2

AWS A5.5 E8018-B2

Kufotokozera: R306Fe ndi pearlitic chitsulo chosagwira magetsi electrode ndi chitsulo ufa ndi otsika hydrogen potaziyamu mtundu zokutira muli 1% Cr - 0.5% Mo. Onse AC ndi DC angagwiritsidwe ntchito, ndipo akhoza welded m'malo onse ndi yochepa arc ntchito.The preheating wa weldment ndi kutentha interlayer ndi 160 ~ 250 °C pa kuwotcherera.

Ntchito: Ntchito kuwotcherera wa 1% Cr - 0.5% Mo pearlitic kutentha zosagwira zitsulo (monga 15CrMo), monga boiler Kutentha pamwamba mapaipi ndi kutentha ntchito pansi 550 ° C, mapaipi nthunzi ndi zotengera kuthamanga ndi kutentha ntchito pansi pa 520 ° C , etc. Angagwiritsidwe ntchito kuwotcherera wa 30CrMnSi castings zitsulo.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

1.00 ~ 1.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Mtengo (J)

Normal Temp.

Zotsimikizika

≥540

≥440

≥47

≥27

Kuyesedwa

550 ~ 640

≥450

20-28

105 ~ 150

 

Kuphatikizika kwa haidrojeni muzitsulo zoyikidwa: ≤6.0mL/100g (njira ya glycerin)

 

Kuwunika kwa X-ray: Ndimapanga

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

3.2

4.0

5.0

Welding Current

(A)

100 ~ 130

140 ~ 180

180 ~ 210

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 350 ℃ isanayambe ntchito yowotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, sikelo yamafuta, madzi, ndi zonyansa pazigawo zowotcherera musanayambe kuwotcherera.