Ni102 (AWS ENi-1) ndi electrode yeniyeni ya nickel yokhala ndi titaniyamu-calcium. Ingagwiritsidwe ntchito powotcherera malo onse ndi AC ndi DC.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Aloyi wa Nickel ndi NickelkuwotchereraElekitirodi

Ni102                                                     

GB/T ENi2061

AWS A5.11 ENi-1

Kufotokozera: Ni102 ndi electrode yeniyeni ya nickel yokhala ndi titaniyamu-calcium. Ingagwiritsidwe ntchito powotcherera malo onse ndi AC ndi DC. Chitsulo chosungidwacho chili ndi mphamvu zabwino zamakaniko, kukana kutentha komanso kukana dzimbiri.

Kugwiritsa Ntchito: Kugwiritsidwa ntchito polumikiza nikeli yoyera (UNS N02200 kapena N02201) popanga ndi kuyika zitsulo, kulumikiza chitsulo chopangidwa ndi nikeli, kuyika pamwamba pa chitsulo ndi kulumikiza chitsulo chosiyana.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Fe

P

S

Si

Al

Ti

Ni

Cu

Zina

≤0.10

≤0.7

≤0.7

≤0.020

≤0.015

≤1.2

≤1.0

1.0 ~ 4.0

≥92.0

≤0.2

≤0.5

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Mphamvu yobereka

Mpa

Kutalikitsa

%

Chotsimikizika

≥410

≥200

≥18

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.5

3.2

4.0

kuwotchereramagetsi

(A)

50 ~ 80

80 ~ 120

130 ~ 170

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 350℃ isanayambe kuwotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, mafuta, madzi, ndi zinyalala pa zipangizo zolumikizira musanagwiritse ntchito.

 