Electrode ikuyika chitsulo chosungunula cha 65Ni-20Cr-2Nb-1.5Mo.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

EN ISO CODE: 14172:ENi6082

Electrode ikuyika chitsulo chosungunula cha 65Ni-20Cr-2Nb-1.5Mo. Chitsulo chosungunula chapamwamba kwambiri. Ndi choyenera kwambiri pa zitsulo zosungunula zokhala ndi zinthu zofanana ndi zawo, pazitsulo zophimba pamwamba ndi aloyi ya Nickel-Chromium-Iron pamene zinthu zambiri za Manganese sizikuwononga, pazitsulo zosungunula za Nickel Chromium-Iron ndi zitsulo zosiyanasiyana. Ndi yoyenera kuphimba mbale za forge. Ndibwino kwambiri pakusungunula zitsulo za 9% Ni kuti zigwiritsidwe ntchito powunda. Imagwiritsidwanso ntchito pakuwunda zitsulo za Nickel-Chromium zomwe zimagwiritsidwa ntchito pa kutentha kwambiri monga zinthu zotenthetsera ng'anjo ndi machubu okonzanso.

CHITSULO CHONSE CHOMWE CHIMANGOPANGIDWA NDI MANKHWALA OMWE ALI BWINO KWAMBIRI

Chinthu C Mn Si Cr Ni Fe Nb Cu Ti S P
Peresenti ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

Katundu Wamba wa Makina a Chitsulo Chosenda

UTS YS Kutalikitsa Mphamvu ya CVN (J) Kukula kwa Mbali Mphamvu Yokwera pa
(MPa) (MPa) (L = 5d)% pa Osachepera 196°C pa kutentha kochepera 196°C (mm) 600°C kwa maola 1000.
620 500 30 75 0.85 160 MPa

DATA LACHINSINSI NDI LOPAKITSA: DC (+)

Kukula (mm)

Kutalika kwa Dia x

5×350

4×350

3.15×350

2.5×350

Mitundu Yamakono (Amps)

150-180

120-150

80-110

60-70

Kulemera/Katoni (kgs)

2.5

2.5

2.5

2.5

Chenjezo

1. Onetsetsani kuti ma electrode ndi ouma. Umitsaninso ma electrode pa 300-325°C kwa ola limodzi.

2. Sungani mzere waufupi, wopindika komanso chepetsani kutentha komwe kumalowa.

3. Lolani chotenthetsera chizizire mpaka pansi pa 50 C musanachiike, onjezerani gawo lotsatira.