AWS ENi-C1 (Z308) ndi elekitirodi yachitsulo chopangidwa ndi chitsulo chochepa cha carbon core komanso zokutira zolimba za graphitized.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Cast Iron Welding Electrode

Z308                                                     

GB/T EZNi-1

AWS A5.15 EN-C1

Description: Z208 ndi elekitirodi chitsulo chotayidwa ndi otsika mpweya zitsulo pachimake ndi ❖ kuyanika amphamvu graphitized.Itha kugwiritsidwa ntchito pa AC ndi DC.Chowotchereracho chimatha kukhala chitsulo chotuwa chikazizira pang'onopang'ono, koma kukana kwake kukakhala kocheperako.

Ntchito: Amagwiritsidwa ntchito kukonza zolakwika pamiyendo yachitsulo yotuwa.

 

Chemical zikuchokera weld zitsulo (%):

C

Si

Mn

S

Ni

Fe

Ena

≤2.0

≤2.5

≤1.0

≤0.03

≥90

≤8.0

≤1.0

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

2.5

3.2

4.0

Welding panopa

(A)

65-90

90-110

120 ~ 150

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 150 ℃ isanayambe ntchito yowotcherera;

2. Kupsyinjika mu malo okonzera kuwotcherera kumatha kuthetsedwa mwa kugwedeza weld kuti apewe ming'alu.

 

 

Wenzhou Tianyu Electronic Co., Ltd. unakhazikitsidwa mu 2000. Takhala chinkhoswe kupanga maelekitirodi kuwotcherera, ndodo kuwotcherera, ndi consumables kuwotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 