AWS ER309Si Stainless Steel Welding Waya MIG ndi TIG Welding Ndodo Filler Ndodo

Kufotokozera Kwachidule:

Waya wowotcherera chitsulo chosapanga dzimbiri ali ndi luso lapamwamba kwambiri, kuwotcherera kwaukadaulo kwaukadaulo wamagawo onse.Amagwiritsidwa ntchito kwambiri m'makampani: zomangamanga, magalimoto, zomangamanga, makina amigodi, njanji, chitoliro chamafuta, zida zonyamula mpweya, zida zamagetsi, ndi zina zambiri.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Gulu la AWS: AWS 5.9

MALANGIZO:

Waya wowotcherera chitsulo chosapanga dzimbiri ali ndi luso lapamwamba kwambiri, kuwotcherera kwaukadaulo kwaukadaulo wamagawo onse.Amagwiritsidwa ntchito kwambiri m'makampani: kapangidwe kanyumba, galimoto, uinjiniya wa mlatho, makina amigodi, njanji, chitoliro chamafuta, zida zonyamula mpweya, zida zamagetsi, etc.

CHITSANZO NO.& SIZE:

1. Fakitale kupereka OEM utumiki.

2. Chitsanzo: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi etc.

3. Kukula kwa waya wa MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4.TIG waya kukula: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm .

MAU OYAMBA:

Timapereka mitundu yosiyanasiyana ya waya wowotcherera zitsulo zosapanga dzimbiri, kuphatikiza waya wowotcherera wa Mig, waya wowotcherera ndodo ya Tig ndi waya wowotcherera wa arc, zonse zapamwamba kwambiri ndipo zimagulitsidwa padziko lonse lapansi.

Kupatula 308 ndi 309, timaperekanso 304, 321, 347, 316L, 310, 2209, ndi 201. Komanso zizindikiro zapadera monga 318L, 904L, 2594, NiCrMo-3, Ni1.

KUPAKA:

Waya wowotcherera wa Mig (paketi ya spool ndi ng'oma)

Kutalika: 0.8-2.0mm

Phukusi: 1 kg / spool, 5 kg / spool, 15 kg / spool, 20 kg / spool, 100 kg / drum, 200 kg / drum

Kuyika waya wowotcherera ndodo (machubu apulasitiki)

Kutalika: 1.0-5.0mm

Phukusi: 5 kg / paketi

Waya wowotcherera arc pansi pamadzi

Kutalika: 2.5-5.0mm

Phukusi: 20kg / paketi, 25kg / paketi

Kupaka kwapakatikati ndi OEM ndizolandiridwa!

NTCHITO ZA CHEMICAL ZA WAYA WOSANGALATSA ZITSWIRI WOWOCHERA:

Chitsanzo No.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304l pa

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

Mtengo wa ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

Mtengo wa ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

Mtengo wa ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

Mtengo wa ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

Mtengo wa ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

Mtengo wa ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

Mtengo wa ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

Mtengo wa ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

Mtengo wa ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

Mtengo wa ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

Mtengo wa ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

Mtengo wa ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

ZINTHU ZOCHITIKA ZA WAYA WOKUTENGA:

Chitsanzo No.

Tensile mphamvu Rm (Mpa)

Kutulutsa mphamvu Rel kapena Rp0.2(Mpa)

Elongation

(%)

Chitsanzo No.

Tensile mphamvu Rm (Mpa)

Kutulutsa mphamvu Rel kapena Rp0.2(Mpa)

Elongation

(%)

304

550

--

25

Mtengo wa ER309LSi

510

320

25

304l pa

510

--

25

Mtengo wa ER316

510

320

25

Mtengo wa ER307

590

350

25

ER316L

510

320

25

Mtengo wa ER308

550

350

25

Mtengo wa ER316LSi

510

320

20

ER308L

510

320

25

Mtengo wa ER310

550

350

25

Mtengo wa ER308LSi

510

320

25

Mtengo wa ER347

550

350

25

Mtengo wa ER309

550

350

25

Mtengo wa ER317

550

350

25

Mtengo wa ER309L

510

320

25

Mtengo wa ER321

550

350

25

TIG ndi MIG zitsulo zosapanga dzimbiri zowotcherera mawaya

YB5092-2005

AWS

Chemical Composition%

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

Mtengo wa ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

Mtengo wa ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

Mtengo wa ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

Mtengo wa ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

Mtengo wa ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

Mtengo wa ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

Mtengo wa ER316

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

Mtengo wa ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

Chithunzi cha H08Cr19Ni12Mo2Nb

Mtengo wa ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

Zithunzi za H07Cr20Ni34Mo2Cu3Nb

Mtengo wa ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nd0.7

Zithunzi za H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nd0.35

Chithunzi cha H08Cr20Ni10Ti

Mtengo wa ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

Chithunzi cha H08Cr21 Ni10Nb

Mtengo wa ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

Mtengo wa ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

Mtengo wa ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

ku 1.80

Chithunzi cha H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

Mtengo wa ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

Mtengo wa ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

Chithunzi cha H03Cr24Ni13MoL

Mtengo wa ER309L

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

Chithunzi cha H05Cr17Ni4Cu4Nb

Mtengo wa ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

ku;3 Nb;0.28

H08Cr26Ni5Mo2

Mtengo wa ER453

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

Chithunzi cha H05Cr22Ni11Mn6Mo3VN

Mtengo wa ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Wenzhou Tianyu Electronic Co., Ltd. unakhazikitsidwa mu 2000. Takhala chinkhoswe kupanga maelekitirodi kuwotcherera, ndodo kuwotcherera, ndi consumables kuwotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 

Wenzhou Tianyu Electronic Co., Ltd. unakhazikitsidwa mu 2000. Takhala chinkhoswe kupanga maelekitirodi kuwotcherera, ndodo kuwotcherera, ndi consumables kuwotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.