Waya Wowotcherera wa AWS ER5183 Aluminiyamu Wowotcherera Ndodo Zowotcherera za Aluminiyamu MIG ndi Waya wa Tig

Kufotokozera Kwachidule:

ER5183 ndi yoyenera kulumikiza MIG ndi aluminiyamu magnesium alloy kuti mphamvu yokoka ikhale yokwera kwambiri ndipo ngati chitsulo choyambira ndi 5083 kapena 5654 mphamvu yokoka ingakhale yokwera kwambiri. Imagwiritsidwa ntchito kwambiri polumikiza kapangidwe ka aluminiyamu magnesium alloy ya zombo, nsanja za m'mphepete mwa nyanja, ma locomotives & magaleta, magalimoto, makontena, zombo zodzaza ndi cryogenic ndi zina zotero.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

ER5183 ndi yoyenera kulumikiza MIG ndi aluminiyamu magnesium alloy, ndipo ngati chitsulo choyambira chili 5083 kapena 5654, mphamvu yokoka ingakhale yokwera kwambiri. Imagwiritsidwa ntchito kwambiri polumikiza zinthu zopangidwa ndi aluminiyamu magnesium alloy za sitima, nsanja za m'mphepete mwa nyanja, ma locomotives ndi magaleta, magalimoto, makontena, zombo zodzaza ndi madzi ndi zina zotero. Chitsulo chake chosungunula chimatha kupirira dzimbiri la madzi amchere.

Malo Owotcherera: F, HF, V

Mtundu wa Zamakono: DCEP

CHIDZIWITSO:

Kusunga phukusi la waya bwino musanagwiritse ntchito.

Malo onse awiri omwe akulumikizidwa ndi weldment ndi waya ayenera kutsukidwa kuchotsa zinyalala za kuipitsidwa ndi mafuta, zokutira za oxide, chinyezi ndi zina zotero.

Kuti chitsulo chiwoneke bwino, ndikofunikira kutenthetsa chitsulocho mpaka 100℃-200℃ musanachiwotche ngati makulidwe ake ndi 10mm kapena kuposerapo.

Ndi bwino kuyika chidebe chaching'ono pansi pa malo olumikizira zitsulo kuti chithandizire chitsulo chosungunuka kuti chizilowa bwino muzitsulozo.

Malinga ndi malo owetera ndi makulidwe a chitsulo choyambira, mpweya woteteza uyenera kusankhidwa, monga 100%Ar, 75%Ar+25%He, 50%Ar+50%He, ndi zina zotero.

Mikhalidwe yolumikizira yomwe yatchulidwa pamwambapa ndi yabwino kwambiri ndipo ndi bwino kuchita chiyeneretso cha njira yolumikizira malinga ndi polojekiti musanayiyike mu njira yolumikizira yovomerezeka.

ER5183 KUPANGIDWA KWA KHEMIKALI KWA CHITSULO CHOMWE CHAKHALA (%):

SI FE CU MN MG CR ZN TI AI BE
Muyezo ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Kulinganiza ≤0.0003
Zachizolowezi 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Kulinganiza 0.0001

KATUNDU WA MAKANIKO WA CHITSULO CHOMWE CHABEDWA (AW):

MPA YA MPHAMVU YA KUKONGOLA (MPA) MPA (MPA) YA MPAMVU YOPANGIDWA KULEMERA A4 (%)
Zachizolowezi 280 150 18

Kukula ndi Mphamvu Yoyenera ya MIG (DC+):

CHIDULE CHA WAYA WOPULUMUTSA (MM) 1.2 1.6 2.0
Kuwotcherera Mphamvu (A) 180-300 200-400 240-450
Kuwotcherera Voltage (V) 18-28 20-20 22-34

Kukula ndi Mphamvu Yoyenera ya TIG (DC¯):

CHIDULE CHA WAYA WOPULUMUTSA (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Kuwotcherera Mphamvu (A) 150-250 200-320 220-400

 

 

Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 

 