ER5356 Aluminium Welding Waya Wowotcherera Ndodo ndi Electrodes

Kufotokozera Kwachidule:

ER5356 ndi aloyi ya aluminiyamu yomwe imagwiritsidwa ntchito nthawi zonse yomwe imasankhidwa chifukwa cha mphamvu zake zometa ubweya wambiri.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

ER5356 ndi aloyi ya aluminiyamu yomwe imagwiritsidwa ntchito nthawi zonse yomwe imasankhidwa chifukwa cha mphamvu zake zometa ubweya wambiri.Kuphatikiza apo, imaperekanso kukana kwa dzimbiri kwabwino kwambiri mukakumana ndi madzi amchere.ER5356 iyenera kuganiziridwa pakuwotcherera 5000 mndandanda wazitsulo zotayidwa.

Zomwe Zimagwira Ntchito: Waya Wowotcherera Wodzaza

Gawo la AWS: ER5356 Chitsimikizo: AWS A5.10/ A5.10M:1999
Aloyi: ER5356 AWS/ASME SFA A5.10
Malo Welding:
F, V, O, H
Panopa:
Chithunzi cha DCEP-GMAW
AC-GTAW
Zofananira (monga welded)
Conductivity: 29% IACS (-0)/27% IACS (-H18)
Kuthamanga Kwambiri, kpsi: 38
Mtundu: Choyera
Melting Point 1175⁰F Kukhazikika 1060⁰F Kuchulukana 0.096 lbs/cu In.
Ma Wire Chemistry monga pa AWS A5.10 (miyezo imodzi ndiyokwera kwambiri)
Si Fe Cu Mn Mg Cr Zn Ti Zina AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Zotsalira
Zowotcherera Zofananira
Diameter Njira Volt Amps GESI
in (mm)
.030 (.8) Mtengo wa GMAW 15-24 60-175 Argon (cfh)
.035 (.9) Mtengo wa GMAW 15-27 70-185 Argon (cfh)
3/64 " (1.2) Mtengo wa GMAW 20-29 125-260 Argon (cfh)
1/16 " (1.6) Mtengo wa GMAW 24-30 170-300 Argon (cfh)
3/32 " (2.4) Mtengo wa GMAW 26-31 275-400 Argon (cfh)
Diameter Njira Volt Amps GESI
in (mm)
1/16 " (1.6) Mtengo wa GTAW 15 60-80 Argon (cfh)
3/32 " (2.4) Mtengo wa GTAW 15 125-160 Argon (cfh)
1/8 " (3.2) Mtengo wa GTAW 15 190-220 Argon (cfh)
5/32 " (4.0) Mtengo wa GTAW 15 200-300 Argon (cfh)
3/16 " (4.8) Mtengo wa GTAW 15-20 330-380 Argon (cfh)

Wenzhou Tianyu Electronic Co., Ltd. unakhazikitsidwa mu 2000. Takhala chinkhoswe kupanga maelekitirodi kuwotcherera, ndodo kuwotcherera, ndi consumables kuwotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 

 