AWS/ASME A 5.3 E4043 Aluminium Welding Electrodes

Kufotokozera Kwachidule:

L109 (AWS/ASME A 5.3 E 4043) ndi electrode yoyera ya aluminiyamu yokhala ndi zokutira zokhala ndi mchere.Gwiritsani ntchito DCEP (mwachindunji panopa electrode positive).Yesani kugwiritsa ntchito arc yayifupi kuti muwotchere.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Aluminiyamu ndi Aluminiyamu Aloyi Electrode

L109                                                     

GB/T E1100

AWS A5.3 E1100

Kufotokozera: L109 ndi electrode yoyera ya aluminiyamu yokhala ndi zokutira zokhala ndi mchere.Gwiritsani ntchito DCEP (mwachindunji panopa electrode positive).Yesani kugwiritsa ntchito arc yayifupi kuti muwotchere.

Ntchito: Amagwiritsidwa ntchito kuwotcherera mbale za aluminiyamu ndi zotengera zoyera za aluminiyamu.

Chemical zikuchokera weld zitsulo (%):

Si+Fe

Cu

Mn

Zn

Al

Zina

≤0.95

0.05 ~ 0.20

≤0.05

≤0.10

≥99.0

≤0.15

 

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zotsimikizika

≥80

 

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

3.2

4.0

5.0

Welding panopa

(A)

80-100

110 ~ 150

150 ~ 200

 

Zindikirani:

1. Elekitirodi ndi yosavuta kukhudzidwa ndi chinyezi, choncho iyenera kusungidwa mu chidebe chowuma chopanda mpweya kuti zisawonongeke chifukwa cha chinyezi;electrode iyenera kuphikidwa pafupifupi 150 ° C kwa maola 1 mpaka 2 musanayambe kuwotcherera;

2. Mbale zogwirizira ziyenera kugwiritsidwa ntchito musanawotchere, ndipo kuwotcherera kuyenera kuchitidwa pambuyo potenthetsa mpaka 200 ~ 300 ° C malinga ndi makulidwe a weld;ndodo yowotcherera iyenera kukhala yozungulira pamwamba pa kuwotcherera, arc iyenera kukhala yaifupi momwe zingathere, ndipo m'malo mwa ndodo zowotcherera ziyenera kuchitika mwamsanga;

3. Kuwotcherera kuyenera kutsukidwa ndi mafuta ndi zonyansa musanayambe kuwotcherera, ndipo slag iyenera kuchotsedwa mosamala pambuyo pa kuwotcherera, ndikutsuka ndi nthunzi kapena madzi otentha.

 

Wenzhou Tianyu Electronic Co., Ltd. unakhazikitsidwa mu 2000. Takhala chinkhoswe kupanga maelekitirodi kuwotcherera, ndodo kuwotcherera, ndi consumables kuwotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 


  • Zam'mbuyo:
  • Ena: