Waya Wowotcherera wa ER4043 Aluminiyamu ndi Aluminiyamu Wowotcherera Waya Wowotcherera wa Tig ndi Mig

Kufotokozera Kwachidule:

ER4043 ndi waya wowotcherera wa aluminiyamu wogwiritsidwa ntchito kwambiri. Ndi imodzi mwa waya wakale kwambiri komanso wogwiritsidwa ntchito kwambiri wowotcherera ndi wopangira zitsulo.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

ER4043 ndi waya wowotcherera wa aluminiyamu wogwiritsidwa ntchito kwambiri. Ndi imodzi mwa zitsulo zakale kwambiri komanso zogwiritsidwa ntchito kwambiri zowotcherera ndi zomangira. Chitsulo cha aluminiyamu ichi chili ndi zowonjezera za silicon, zomwe zimapangitsa kuti dziwe lowotcherera liziyenda bwino komanso zimapangitsa kuti dziwe lowotcherera lisamavutike kwambiri ndi ming'alu. Kumapeto kwake kowala kwa weld kumapangitsa kuti ikhale yosankhidwa ndi owotcherera otchuka. ER4043 ingagwiritsidwe ntchito kuwotcherera mitundu yosiyanasiyana ya aluminiyamu.

Ntchito Zachizolowezi: waya wothira welding; waya wopopera ndi wopangira zitsulo wa lawi

Kalasi ya AWS: ER4043 Chitsimikizo: AWS A5.10/ A5.10M:1999
Aloyi: ER4043 AWS/ASME SFA A5.10

 

Kuwotcherera Udindo:
F, V, OH, H
Zamakono:
DCEP-GMAW
AC-GTAW

 

Katundu Wamba (monga momwe zimagwiritsidwira ntchito)

Kuyendetsa bwino kwa magetsi: 42% IACS (-12)
Mphamvu Yokoka, kpsi: 29
Mtundu: Imvi
Malo Osungunuka 1170⁰F Kukhazikika 1065⁰F Kuchulukana 0.097 lbs/cu Mu.

Mankhwala a Waya Omwe Amagwiritsidwa Ntchito Mogwirizana ndi AWS A5.10 (mtengo umodzi ndi wapamwamba kwambiri)

Si Fe Cu Mn Mg Zn Ti Zina Al
4.5-6.0 0.8 0.30 0.05 0.05 0.10 0.20 0.15 Chotsalira
Magawo Omwe Amawotcherera Achizolowezi
M'mimba mwake Njira Volti Ma Amps GESI
in (mm)
.030 (.8) GMAW 15-24 60-175 Argon (cfh)
.035 (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argon (cfh)
M'mimba mwake Njira Volti Ma Amps GESI
in (mm)
1/16” (1.6) GTAW 15 60-80 Argon (cfh)
3/32” (2.4) GTAW 15 125-160 Argon (cfh)
1/8” (3.2) GTAW 15 190-220 Argon (cfh)
5/32” (4.0) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

 

Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 

 