Zitsulo Zodzaza ndi CARBON STEEL ER70S-3 za Kuwetera Arc Yotetezedwa ndi Gasi

ER70S3 ndi waya wa MIG wogwiritsidwa ntchito kwambiri womwe umagwiritsidwa ntchito powotcherera zitsulo za kaboni. Ndi waya wa silicon ndi manganese deoxidized womwe umapangitsa kuti ukhale wabwino kwambiri popanga zinthu zambiri. Chogulitsachi chimafuna mpweya woteteza.

Ntchito Zachizolowezi: kupanga zinthu wamba, mipando yachitsulo, chitsulo chapepala, kupanga zinthu zokongoletsera zachitsulo, zida zapafamu

Kalasi ya AWS: ER70S3 Chitsimikizo: AWS A5.18/A5.18M: 2005
Aloyi: ER70S3 ASME SFA A5.18

 

Malo Owotcherera: F, V, OH, H Zamakono:
MIG-DCEP
TIG-DCEN

 

Mphamvu Yokoka, kpsi: 70
Mphamvu Yopereka, kpsi: 58
Kutalika kwa 2”%: 22

Mankhwala a Waya Omwe Amagwiritsidwa Ntchito Mogwirizana ndi AWS A5.18 (Mitengo imodzi ndiyo yokwanira)

C Mn Si P S Ni Cr Mo V Cu
0.06-0.15 0.90-1.40 0.45-0.75 0.025 0.035 0.15 0.15 0.15 0.03 0.50
Magawo Omwe Amawotcherera Achizolowezi
M'mimba mwake Njira Volti Ma Amps Mpweya Woteteza
in (mm)
.035 (0.9) GMAW 28-32 165-200 Kutumiza kwa Spray 98% Argon + 2% Oxygen kapena 75% Argon + 25% CO2
.045 (1.2) GMAW 30-34 180-220 Kutumiza kwa Spray 98% Argon + 2% Oxygen kapena 75% Argon + 25% CO2
1/16 (1.6) GMAW 30-34 230-260 Kutumiza kwa Spray 98% Argon + 2% Oxygen kapena 75% Argon + 25% CO2
.035 (0.9) GMAW 22-25 100-140 Kusamutsa Kozungulira Kafupi 100% CO2 kapena 75% Argon +25% CO2
.045 (1.2) GMAW 23-26 120-150 Kusamutsa Kwafupipafupi 100% CO2 kapena 75% Argon +25% CO
1/16 (1.6) GMAW 23-26 160-200 Kusamutsa Kwafupipafupi 100% CO2 kapena 75% Argon +25% CO
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon

 