Carbon Steel Welding Electrode AWS A5.1 E7018-1 Low Hydrogen Welding Rods

Kufotokozera Kwachidule:

J501Fe (AWS E7018-1) ndi electrode yachitsulo ya carbon ndi ufa wachitsulo ndi zokutira zochepa za hydrogen potassium.AC ndi DC angagwiritsidwe ntchito kuwotcherera onse malo.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Carbon Steel WeldingElectrode

J506Fe-1

GB/T E5018-1

AWS A5.1 E7018-1

Kufotokozera: J501Fe ndi electrode ya carbon steel yokhala ndi ufa wachitsulo ndi zokutira zochepa za hydrogen potaziyamu.AC ndi DC angagwiritsidwe ntchito kuwotcherera onse malo.Makhalidwe ake ndikuti ❖ kuyanika kumakhala ndi ufa wachitsulo wokhala ndi ntchito yabwino kwambiri yowotcherera.Chitsulo choyikidwa chimakhala ndi mphamvu yabwino yolimba.

Ntchito: Iwo ntchito kuwotcherera mpweya zitsulo ndi otsika aloyi zitsulo lolingana mphamvu kalasi, monga Q345, Q345R, etc.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

S

P

≤0.12

≤1.60

≤0.70

≤0.030

≤0.035

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Mtengo (J)

(-46 ℃)

Zotsimikizika

≥490

≥400

≥22

≥27

Kuyesedwa

520 ~ 580

≥410

24-30

50 ~ 100

 

Kuphatikizika kwa haidrojeni muzitsulo zoyikidwa: ≤4.0mL/100g (njira ya glycerin)

 

Kuwunika kwa X-ray: Ndimapanga

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

2.5

3.2

4.0

5.0

5.8

Welding panopa

(A)

90-120

120 ~ 150

170 ~ 200

210 ~ 250

240 ~ 310

 

Zindikirani:

1.The elekitirodi ayenera kuphika kwa ola 1 pa 350 ℃ pamaso kuwotcherera ntchito;

2. Ndikofunikira kuyeretsa dzimbiri, sikelo yamafuta, madzi, ndi zonyansa pazigawo zowotcherera musanawotchere;

 

Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelectrode kuwotchereras, ndodo zowotcherera, ndi zinthu zowotcherera kwa zaka zopitilira 20.

Zogulitsa zathu zazikulu zimaphatikizapo zitsulo zosapanga dzimbirielectrode kuwotchereras, mpweya zitsulo kuwotcherera maelekitirodi, low aloyi kuwotcherera maelekitirodi, surfacing ma elekitirodi kuwotcherera, faifi tambala & cobalt aloyi kuwotcherera maelekitirodi, wofatsa zitsulo & otsika aloyi mawaya kuwotcherera, zitsulo zosapanga dzimbiri kuwotcherera mawaya, mpweya wotetezedwa flux cored mawaya, aluminium kuwotcherera mawaya, kumizidwa arc kuwotcherera .mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 

 


  • Zam'mbuyo: