Chitsulo Chochepa Choyeretsera Ma Electrode AWS E7018-G Choyeretsera Ndodo Mphamvu ya Chitsulo ndi Hydrogen Yochepa

Kufotokozera Kwachidule:

J507FeNi (AWS E7018-G) ndi electrode yachitsulo chopanda aloyi yokhala ndi ufa wachitsulo ndi zokutira zochepa za haidrojeni. Ingagwiritsidwe ntchito powotcherera malo onse ndi AC ndi DC


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Low Aloyi Zitsulo kuwotcherera elekitirodi

J507FeNi                                                    

GB/T E5018-G

AWS E7018-G

Kufotokozera: J507FeNi ndi electrode yachitsulo chopanda aloyi yokhala ndi ufa wachitsulo komanso chophimba chochepa cha haidrojeni. Ingagwiritsidwe ntchito powotcherera malo onse ndi AC ndi DC. Kukhazikika kwa magwiridwe antchito a kuwotcherera kwa AC ndi kochepa poyerekeza ndi kwa kuwotcherera kwa DC

Kugwiritsa Ntchito: Kugwiritsidwa ntchito kuwotcherera zitsulo zapakati pa kaboni ndi zitsulo zotsika kutentha, monga 16MnDR, ndi zina zotero.

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Ni

S

P

≤0.08

0.80 ~ 1.30

≤0.65

1.20 ~ 2.00

≤0.030

≤0.030

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

 

Kulimba kwamakokedwe

Mpa

 

Mphamvu yobereka

Mpa

 

Kutalikitsa

%

 

Mtengo wa zotsatira (J)

-40℃

Chotsimikizika

≥490

≥390

≥22

≥54

 

Kuchuluka kwa haidrojeni m'chitsulo chosungidwa: ≤6.0mL/100g (njira ya glycerin)

Kuwunika kwa X-ray: Giredi I

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo
(mm)

3.2

4.0

5.0

kuwotcherera Current

(A)

90 ~ 120

140 ~ 180

170 ~ 210

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 350℃ isanayambe kuwotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, mafuta oyeretsera, madzi, ndi zinyalala pa zipangizo zowotcherera musanawotchetse.

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotcherera, ndi zogwiritsidwa ntchito zowotcherera kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode odulira zitsulo zosapanga dzimbiri, ma electrode odulira zitsulo za kaboni,ma electrode otsika a alloy welding, maelekitirodi olumikizira pamwamba, maelekitirodi olumikizira a nickel & cobalt alloy, mawaya olumikizira achitsulo chofatsa & low alloy, mawaya olumikizira achitsulo chosapanga dzimbiri, mawaya olumikizira a flux otetezedwa ndi gasi, mawaya olumikizira a aluminiyamu, mawaya olumikizira a arc olowa pansi. mawaya, mawaya olumikizira a nickel & cobalt alloy, mawaya olumikizira a mkuwa, mawaya olumikizira a TIG & MIG, maelekitirodi a tungsten, maelekitirodi olumikizira kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 