Ndodo Yowotcherera ya AWS E10015-G (J707Ni) Yokhala ndi Chitsulo Chochepa Cho ...

Kufotokozera Kwachidule:

J707Ni (AWS E10015-G) ndi electrode yachitsulo yolimba kwambiri yokhala ndi chitsulo chopanda hydrogen sodium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Low AloyiKuwotcherera kwa ZitsuloElekitirodi

J707Ni                               

GB/T E7015-G

AWS E10015-G

 

Kufotokozera: J707Ni ndi electrode yachitsulo yolimba kwambiri yokhala ndi chofunda chochepa cha sodium. Gwiritsani ntchito DCEP (electrode ya direct current positive) ndipo imatha kulumikizidwa m'malo onse. Chitsulo chosungidwa chili ndi mphamvu zabwino zamakanika. Poyerekeza ndi electrode ya J707, chinthu chachikulu cha J707Ni ndikuti kulimba kwa kutentha kochepa komanso kukana ming'alu kwawonjezeka kwambiri.

Kugwiritsa Ntchito: Kugwiritsidwa ntchito powotcherera zitsulo zolimba zotsika kwambiri zokhala ndi mphamvu zofanana, monga 14MnMoVB, WEL-TEN70 ndi Japanese HW56 ndi zitsulo zina zolimba zotsika kwambiri.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Si

Mn

Ni

Mo

Cr

S

P

≤0.10

≤0.60

≥1.00

1.80 ~ 2.20

0.40 ~ 0.60

≤0.20

≤0.030

≤0.030

 

Kapangidwe ka makina a chitsulo chosungunula:

 

Chinthu choyesera

 

Kulimba kwamakokedwe

Mpa

 

Mphamvu yobereka

Mpa

 

Kutalikitsa

%

 

Mtengo wa zotsatira (J)

-40℃

-50℃

 

Chotsimikizika

≥690

≥590

≥15

—

≥27

 

Yayesedwa

760

630

23

140

—

 

 

Kuchuluka kwa haidrojeni m'chitsulo chosungidwa: ≤4.0mL/100g (njira ya glycerin) 

Kuyang'anira X-ray: Giredi I

 

Mphamvu yovomerezeka:

(mm)

M'mimba mwake wa ndodo

2.5

3.2

4.0

5.0

(A)

kuwotcherera Current

60 ~ 100

100 ~ 140

140 ~ 190

190 ~ 250

 

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa 350 ~380℃ isanayambe kuwotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, mafuta oyezera, madzi, ndi zinyalala pa zipangizo zowotcherera musanawotchetse;

3. Gwiritsani ntchito njira yochepetsera arc polumikiza. Njira yopapatiza yolumikizira ndi yoyenera.

 


  • Yapitayi: