J607 (AWS E9015-D1) Low Alloy Steel Welding Electrodes High-Strength Steel Electrode

Kufotokozera Kwachidule:

J607 (AWS E9015-D1) ndi electrode yachitsulo yotsika kwambiri yokhala ndi chitsulo chochepa cha hydrogen sodium.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Chitsulo cha Low AlloyKuwotchereraElectrode

J607                                       

GB/T E6015-D1

AWS E9015-D1 

 

Kufotokozera: J607 ndi otsika aloyi mkulu-mphamvu zitsulo electrode ndi otsika-hydrogen sodium zokutira.Gwiritsani ntchito DCEP (mwachindunji panopa ma elekitirodi abwino), ndipo akhoza welded m'malo onse.

Ntchito: Ntchito kuwotcherera sing'anga mpweya zitsulo ndi otsika aloyi mkulu-mphamvu zitsulo nyumba lolingana mphamvu, monga Q420, etc.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Mtengo (J)

-30 ℃

Zotsimikizika

≥590

≥490

≥15

≥27

Kuyesedwa

620 ~ 680

≥500

20-28

≥27

 

Kuphatikizika kwa haidrojeni muzitsulo zoyikidwa: ≤4.0mL/100g (njira ya glycerin) 

Kuwunika kwa X-ray: Ndimapanga

 

Zomwe tikulimbikitsidwa:

(mm)

Ndodo diameter

2.0

2.5

3.2

4.0

5.0

5.8

(A)

KuwotchereraPanopa

60-80

70-90

90-120

140 ~ 180

170 ~ 210

210 ~ 260

 

Zindikirani:

1. Elekitirodi ayenera kuphika kwa ola 1 pa 350 ℃ pamaso kuwotcherera ntchito;

2. Ndikofunikira kuyeretsa dzimbiri, sikelo yamafuta, madzi, ndi zonyansa pazigawo zowotcherera musanawotchere;

3. Gwiritsani ntchito kachipangizo kakang'ono powotcherera.Njira yopapatiza yowotcherera ndiyoyenera.


  • Zam'mbuyo:
  • Ena: